To achieve a safe treatment of arsenic-containing acid wastewater,a new process was proposed,including arsenic removal via sulfide precipitation and hydrothermal mineralization stabilization.Under optimal conditions o...To achieve a safe treatment of arsenic-containing acid wastewater,a new process was proposed,including arsenic removal via sulfide precipitation and hydrothermal mineralization stabilization.Under optimal conditions of sulfide precipitation,99.65%of arsenic from wastewater was precipitated in the form of amorphous As2S3.The As leaching concentration of amorphous As2S3 in TCLP(toxicity characteristic leaching procedure)test was up to 212.97 mg/L,therefore,hydrothermal mineralization was adopted to improve the stability of amorphous As2S3.The results showed that the As leaching concentration of mineralized As2S3 was only 4.82 mg/L.Furthermore,the amorphous As2S3 could be transformed into crystallized As2S3(orpiment)in the presence of mineralizer Na2SO4.Simultaneously,the As leaching concentration of crystallized As2S3 was further reduced to 3.86 mg/L.Hydrothermal mineralization was an effective method for the stabilization of As2S3.Therefore,this process has a greater application in the treatment of arsenic-containing wastewater.展开更多
基金Projects(2018YFC1901601,2018YFC1901604,2018YFC1901605) supported by the National Key Research and Development Program of ChinaProject(201806375047) supported by the Visiting Scholar of China Scholarship CouncilProject(51404296) supported by the Young Scientists Fund of the National Natural Science Foundation of China
文摘To achieve a safe treatment of arsenic-containing acid wastewater,a new process was proposed,including arsenic removal via sulfide precipitation and hydrothermal mineralization stabilization.Under optimal conditions of sulfide precipitation,99.65%of arsenic from wastewater was precipitated in the form of amorphous As2S3.The As leaching concentration of amorphous As2S3 in TCLP(toxicity characteristic leaching procedure)test was up to 212.97 mg/L,therefore,hydrothermal mineralization was adopted to improve the stability of amorphous As2S3.The results showed that the As leaching concentration of mineralized As2S3 was only 4.82 mg/L.Furthermore,the amorphous As2S3 could be transformed into crystallized As2S3(orpiment)in the presence of mineralizer Na2SO4.Simultaneously,the As leaching concentration of crystallized As2S3 was further reduced to 3.86 mg/L.Hydrothermal mineralization was an effective method for the stabilization of As2S3.Therefore,this process has a greater application in the treatment of arsenic-containing wastewater.