In authors’ previous work [Mater. Charact. 141 (2018) 212-222]. it was found that the heterogeneous deformed microstructures can be replaced by the relatively homogeneous recrystallized grains through an annealing tr...In authors’ previous work [Mater. Charact. 141 (2018) 212-222]. it was found that the heterogeneous deformed microstructures can be replaced by the relatively homogeneous recrystallized grains through an annealing treatment. However, there are still some relatively large recrystallized grains. To find the reasons for the formation of large grains, some new annealing treatment tests were done, and the cellular automation (CA) simulations were carried out in the present work. The experimental results showed that the microstructural evolution during annealing treatment is significantly affected by the content of S phase. So. the effects of δ phase on the nucleation and growth of grains are carefully considered in the CA model to accurately simulate the microstructural evolution behavior. By the CA simulation, it is found that the dislocation density rapidly decreases due to the nucleation of static recrystallization (SRX) and the growth of dynamc recrystallization (DRX) nuclei at the early stage of annealing. The high initial dislocation density provide the high velocity for the growth of DRX nuclei, which is responsible for the formation of coarse grains, However, the growth rate of SRX nuclei is relatively small due to the low dislocation density and pinning effects of δ phase.展开更多
TiAlSiN hard coatings were synthesized on high-speed steel using an arc ion enhanced magnetic sputtering hybrid system.The microstructure and hardness of the coatings at different annealing temperatures were explored ...TiAlSiN hard coatings were synthesized on high-speed steel using an arc ion enhanced magnetic sputtering hybrid system.The microstructure and hardness of the coatings at different annealing temperatures were explored by means of XRD,TEM,EDAX and Vickers indentation.The as-deposited TiAlSiN coatings were confirmed to be amorphous due to high depositing rate and low deposition temperature during the film growth.The transformation from amorphous to nanocomposites of nano-crystallites and amorphousness were observed after the annealing treatment,the microstructure of TiAlSiN coatings annealed at 800°C and 1000°C were consisted of crystalline hcp-AlN,fcc-TiN and amorphous phase,however,the coatings were only consisted of fcc-TiN and amorphous phase when annealing at 1100°C and 1200°C.Meanwhile,the formation of Al2O3 was detected on the coating surface after annealing at 1200°C and it indicated the excellent oxidation resistance of the TiAlSiN coatings under the present experimental conditions.Furthermore,the average grain size of the TiAlSiN coatings after high temperature annealing even at 1200°C was less than 30 nm and the size increased with the increasing temperature.However,the hardness of the so-deposited coatings with HV0.2N=3300 dramatically decreased with the increase of temperature and reached nearly to the hardness of TiN coatings with HV0.2N=2300.展开更多
基金supported by the Hunan Provincial Natural Science Foundation of China (No. 2017JJ3380)the National Natural Science Foundation of China (No. 51775564)+3 种基金the State key Laboratory of High Performance Complex Manufacturing (No. zzyjkt2014-01)the Open-End Fund for the Valuable and Precision Instruments of Central South University (No. CSUZC201821)Hebei Iron and Steel Joint Funds (No. E2015209243)the Fundamental Research Funds for the Central Universities of Central South University (No. 153711025)
文摘In authors’ previous work [Mater. Charact. 141 (2018) 212-222]. it was found that the heterogeneous deformed microstructures can be replaced by the relatively homogeneous recrystallized grains through an annealing treatment. However, there are still some relatively large recrystallized grains. To find the reasons for the formation of large grains, some new annealing treatment tests were done, and the cellular automation (CA) simulations were carried out in the present work. The experimental results showed that the microstructural evolution during annealing treatment is significantly affected by the content of S phase. So. the effects of δ phase on the nucleation and growth of grains are carefully considered in the CA model to accurately simulate the microstructural evolution behavior. By the CA simulation, it is found that the dislocation density rapidly decreases due to the nucleation of static recrystallization (SRX) and the growth of dynamc recrystallization (DRX) nuclei at the early stage of annealing. The high initial dislocation density provide the high velocity for the growth of DRX nuclei, which is responsible for the formation of coarse grains, However, the growth rate of SRX nuclei is relatively small due to the low dislocation density and pinning effects of δ phase.
基金supported by the National Natural Science Foundation of China (50671079, 50531060)National Basic Research Program of China (2004CB619302)Program for New Century Excellent Talents in University of China (NCET-04-0934)
文摘TiAlSiN hard coatings were synthesized on high-speed steel using an arc ion enhanced magnetic sputtering hybrid system.The microstructure and hardness of the coatings at different annealing temperatures were explored by means of XRD,TEM,EDAX and Vickers indentation.The as-deposited TiAlSiN coatings were confirmed to be amorphous due to high depositing rate and low deposition temperature during the film growth.The transformation from amorphous to nanocomposites of nano-crystallites and amorphousness were observed after the annealing treatment,the microstructure of TiAlSiN coatings annealed at 800°C and 1000°C were consisted of crystalline hcp-AlN,fcc-TiN and amorphous phase,however,the coatings were only consisted of fcc-TiN and amorphous phase when annealing at 1100°C and 1200°C.Meanwhile,the formation of Al2O3 was detected on the coating surface after annealing at 1200°C and it indicated the excellent oxidation resistance of the TiAlSiN coatings under the present experimental conditions.Furthermore,the average grain size of the TiAlSiN coatings after high temperature annealing even at 1200°C was less than 30 nm and the size increased with the increasing temperature.However,the hardness of the so-deposited coatings with HV0.2N=3300 dramatically decreased with the increase of temperature and reached nearly to the hardness of TiN coatings with HV0.2N=2300.