The Effect of SiO_2 Additive on Super-hydrophilic Property of TiO_2-SiO_2 Thin Film by Sol-gel Method 被引量:1
1
作者 陈文梅 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2001年第3期30-33,共4页
TiO2-SiO2 thin films have been prepared on slide glass substrates by sol-gel method, and the effect of SiO2 additive on photo-generated hydrophilicity of TiO2 thin film was investigated by measuring the contact angle ... TiO2-SiO2 thin films have been prepared on slide glass substrates by sol-gel method, and the effect of SiO2 additive on photo-generated hydrophilicity of TiO2 thin film was investigated by measuring the contact angle of water, the microstructure, the transmittance, the photocatalytic activity and the specific surface area . The results showed that 10mol% of SiO2 additive was the most effective for decreasing contact angle of water. The SiO2 additive of less than 30mol% has a suppressive effect on the crystal growth of anatase in calcinations, resulting in a large surface area. Consequently, the super-hydrophilicity was improved. 展开更多
关键词 sol-gel tio2-sio2 thin films super- hydrophilicity PHOTOCATALYSIS BET
下载PDF
TiO_2/SiO_2复合薄膜的制备及自清洁性能研究 被引量:1
2
作者 张雪琦 王俊凯 +2 位作者 任亚惠 刘刚 刘志锋 《天津城建大学学报》 2016年第6期437-443,共7页
采用溶胶-凝胶(Sol-Gel)法,并结合浸渍—提拉工艺,以钛酸丁酯、正硅酸乙酯为钛源和硅源,无水乙醇为溶剂,制备了稳定的TiO_2和SiO_2溶胶;再根据不同的镀膜顺序,制备出纳米TiO_2/SiO_2复合薄膜.利用扫描电子显微镜(SEM)、紫外-可见分光光... 采用溶胶-凝胶(Sol-Gel)法,并结合浸渍—提拉工艺,以钛酸丁酯、正硅酸乙酯为钛源和硅源,无水乙醇为溶剂,制备了稳定的TiO_2和SiO_2溶胶;再根据不同的镀膜顺序,制备出纳米TiO_2/SiO_2复合薄膜.利用扫描电子显微镜(SEM)、紫外-可见分光光度计、接触角测量仪等对TiO_2/SiO_2复合薄膜的表面形貌、透光性和亲水性能等进行了分析,研究了溶胶浓度、摩尔配合比、镀膜顺序等对复合薄膜结构和自清洁性能的影响.实验结果表明:当溶胶浓度为0.5,mol/L时,按TiO_2/SiO_2/TiO_2/TiO_2(TSTT)镀膜顺序制备的纳米TiO_2/SiO_2复合薄膜,经紫外灯照射1,h后水接触角小至2.5°,表现出超亲水自清洁性能. 展开更多
关键词 溶胶-凝胶法 tio2/sio2复合薄膜 亲水性 自清洁
下载PDF
TiO_2/SiO_2纳米薄膜的光催化活性和亲水性 被引量:29
3
作者 余家国 赵修建 +2 位作者 陈文梅 林立 张艾丽 《物理化学学报》 SCIE CAS CSCD 北大核心 2001年第3期261-264,共4页
通过 sol-gel工艺在钠钙玻璃表面制备了均匀透明的 TiO_2/SiO_2复合纳米薄膜 .实验结果表明 :当 SiO_2添加量较高时 , TiO_2/SiO_2复合纳米薄膜的光催化活性明显降低 ;当 SiO_2添加量较低时 ,TiO_2/SiO_2复合薄膜的光催化活性无明显变... 通过 sol-gel工艺在钠钙玻璃表面制备了均匀透明的 TiO_2/SiO_2复合纳米薄膜 .实验结果表明 :当 SiO_2添加量较高时 , TiO_2/SiO_2复合纳米薄膜的光催化活性明显降低 ;当 SiO_2添加量较低时 ,TiO_2/SiO_2复合薄膜的光催化活性无明显变化 .在 TiO_2薄膜中添加 SiO_2,可以抑制薄膜中 TiO_2晶粒的长大 ,同时薄膜表面的羟基含量增加 ,水在复合薄膜表面的润湿角下降 ,亲水能力增强 .当 SiO_2含量为 10%- 20%(摩尔分数)时获得了润湿角为 0°的超亲水性薄膜 . 展开更多
关键词 复合纳米薄膜 二氧化钛 二氧化硅 溶胶-凝胶工艺 光催化活性 超亲水性
下载PDF
超亲水TiO_2/SiO_2复合薄膜的制备与表征 被引量:28
4
作者 余家国 赵修建 +2 位作者 林立 韩建军 赵青南 《无机材料学报》 SCIE EI CAS CSCD 北大核心 2001年第3期529-534,共6页
通过 sol-gel工艺在普通钠钙玻璃表面制备了均匀透明的 TiO2/SiO2复合薄膜.实验结果表明:在 TiO2薄膜中添加 SiO2,可以抑制薄膜中 TiO2晶粒的长大,同时薄膜表面的羟基含量增加,水在复合薄膜表面的润... 通过 sol-gel工艺在普通钠钙玻璃表面制备了均匀透明的 TiO2/SiO2复合薄膜.实验结果表明:在 TiO2薄膜中添加 SiO2,可以抑制薄膜中 TiO2晶粒的长大,同时薄膜表面的羟基含量增加,水在复合薄膜表面的润湿角下降,亲水能力增强.当 SiO2含量为 10~20 mol%时获得了润湿角为0°的超亲水性薄膜. 展开更多
关键词 复合薄膜 超亲水性 制备 表征 二氧化钛 二氧化硅 钠钙玻璃 表面薄膜 溶胶-凝胶法
下载PDF
Grain Size and Wettability of TiO_2/SiO_2 Photocatalytic Composite Thin Filing 被引量:11
5
作者 Jiaguo Yu, Xiujian Zhao, Jimmy C Yu, Jun Lin (State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070, China Deportment of Chemised The Chinese University of Hong Kong, Hong Kong, 《Rare Metals》 SCIE EI CAS CSCD 2001年第2期81-86,共6页
The uniform transparent TiO2/SiO2 photocatalytic composite thin films are prepared by sol-gel method on the soda lime glass substrates, and characterized by UV-visible spectroscopy, X-ray diffraction (XRD), transmissi... The uniform transparent TiO2/SiO2 photocatalytic composite thin films are prepared by sol-gel method on the soda lime glass substrates, and characterized by UV-visible spectroscopy, X-ray diffraction (XRD), transmission electron microscopy (TEM), BET surface area, FTIR spectroscopy and X-ray photoelectron spectroscopy (XPS). It was found that the addition of SiO2 to TiO2 thin films can suppress the grain growth of TiO2 crystal, increase the hydroxyl content on the surface of TiO2 films, lower the contact angle for water on TiO, films and enhance the hydrophilic property of TiO2 films. The super-hydrophilic TiO2/SiO2 photocatalytic composite thin films with the contact angle of 0((o) under bar) are obtained by the addition of 10%-20% SiO2 in mole fraction. 展开更多
关键词 sol-gel method tio2/sio2 photocatalytic composite thin films grain size WETTABILITY
下载PDF
射频磁控共溅射制备超亲水TiO_2/SiO_2复合薄膜 被引量:3
6
作者 沈杰 沃松涛 +3 位作者 蔡臻炜 崔晓莉 杨锡良 章壮健 《真空科学与技术学报》 EI CAS CSCD 北大核心 2004年第6期415-419,共5页
采用射频磁控共溅射法制备了SiO2 /TiO2 复合薄膜 ,通过控制SiO2 靶与TiO2 靶的溅射时间可调节SiO2 与TiO2 的比例。所制备的SiO2 /TiO2 薄膜为锐钛矿结构。实验结果表明 :SiO2 的掺入降低了SiO2 /TiO2 复合薄膜的光催化能力 ,但却提高... 采用射频磁控共溅射法制备了SiO2 /TiO2 复合薄膜 ,通过控制SiO2 靶与TiO2 靶的溅射时间可调节SiO2 与TiO2 的比例。所制备的SiO2 /TiO2 薄膜为锐钛矿结构。实验结果表明 :SiO2 的掺入降低了SiO2 /TiO2 复合薄膜的光催化能力 ,但却提高了薄膜的亲水性的维持时间。其中 ,掺入 6 %~ 13%SiO2 的SiO2 /TiO2 复合薄膜 ,在紫外光照射 30min ,接触角降到 2° ;停止照射后 ,在 5天内接触角小于 6°。 展开更多
关键词 sio2 共溅射法 tio2薄膜 复合薄膜 接触角 内接 锐钛矿结构 射频 实验结果 照射
下载PDF
漂珠为载体TiO_2/SiO_2膜的制备及性能研究 被引量:2
7
作者 宋成芳 《环境科学与技术》 CAS CSCD 北大核心 2006年第B08期14-15,18,共3页
以漂珠为载体,探索采用液相沉积法制备TiO2/SiO2膜最佳条件。在自制的光催化反应器中,在相同的条件下,以酸性嫩黄和难处理的焦化废水为目标降解物,做了TiO2/SiO2和TiO2两种膜的光催化氧化对比试验。结果表明,与单一TiO2膜比较,以漂珠为... 以漂珠为载体,探索采用液相沉积法制备TiO2/SiO2膜最佳条件。在自制的光催化反应器中,在相同的条件下,以酸性嫩黄和难处理的焦化废水为目标降解物,做了TiO2/SiO2和TiO2两种膜的光催化氧化对比试验。结果表明,与单一TiO2膜比较,以漂珠为载体,采用液相沉积法制备的TiO2/SiO2改性膜具有较高的光催化氧化性能。 展开更多
关键词 液相沉积法 tio2/Si02薄膜 光催化 漂珠
下载PDF
钛金属有机物热解制备TiO_2-SiO_2复合膜及其光催化活性研究 被引量:11
8
作者 陈小泉 古国榜 刘焕彬 《化学学报》 SCIE CAS CSCD 北大核心 2003年第11期1714-1719,共6页
混有一定量SiO2 溶胶的钛金属有机化合物膜液通过旋液成膜法制备前驱物膜 ,经热解得到TiO2 SiO2 复合膜 .于 610℃焙烧 15min所得复合膜 (Ti∶Si =9∶1)经SEM ,XRD ,UV vis和XPS研究表明 ,膜面由 3 0nm× 2 0 0nm大小的晶体粒子组... 混有一定量SiO2 溶胶的钛金属有机化合物膜液通过旋液成膜法制备前驱物膜 ,经热解得到TiO2 SiO2 复合膜 .于 610℃焙烧 15min所得复合膜 (Ti∶Si =9∶1)经SEM ,XRD ,UV vis和XPS研究表明 ,膜面由 3 0nm× 2 0 0nm大小的晶体粒子组成 ,结构致密 ,膜厚约 2 0 0nm ,其可见光透过率为玻璃基质的 80 %,膜表面Ti3 + /OH-的比值为 1 0 6.对不同SiO2 含量的膜液凝胶进行DSC分析显示 ,少量的SiO2 就能显著提高TiO2 锐钛矿型晶相的形成温度 .膜的光催化活性研究表明一定量的Fe3 + 有利于提高膜的光催化活性 ,但是如果以氯化物的形式加入则对光催化反应不利 ,铬的氯化物同样如此 .另外 ,在钛金属有机物热解制备TiO2 SiO2 复合膜中 ,溶胶SiO2 不利于光催化反应 。 展开更多
关键词 钛金属有机物 热解 制备 tio2-sio2 复合膜 光催化活性 二氧化钛 二氧化硅 催化剂
下载PDF