RuS_2 thin films were prepared by the cost-effective chemicalmethod―successive ionic layer adsorption and reaction (SILAR). The structural, optical, andelectrical properties were investigated using X-ray diffraction,...RuS_2 thin films were prepared by the cost-effective chemicalmethod―successive ionic layer adsorption and reaction (SILAR). The structural, optical, andelectrical properties were investigated using X-ray diffraction, scanning electron microscopy,optical transmittance, and electrical resistivity methods. The results indicate that the films arehomogeneous and dense; the structure of the as-deposited films is amorphous and they crystallizeafter annealed at 500℃ for 30 min. The band gap of the as-deposited films is found to be 1.85 eV,and the electrical resistivity of them is in the order of 10~5 Ω·cm.展开更多
基金This work is financially supported by the Tianjin Science and Technology Committee, China (No. F103004).
文摘RuS_2 thin films were prepared by the cost-effective chemicalmethod―successive ionic layer adsorption and reaction (SILAR). The structural, optical, andelectrical properties were investigated using X-ray diffraction, scanning electron microscopy,optical transmittance, and electrical resistivity methods. The results indicate that the films arehomogeneous and dense; the structure of the as-deposited films is amorphous and they crystallizeafter annealed at 500℃ for 30 min. The band gap of the as-deposited films is found to be 1.85 eV,and the electrical resistivity of them is in the order of 10~5 Ω·cm.