Pour point depressants (PPD) are used to improve the theology of waxy crude. The affect of various factors on the theological properties, and the thermal characteristics of waxy crude treated by PPD have been invest...Pour point depressants (PPD) are used to improve the theology of waxy crude. The affect of various factors on the theological properties, and the thermal characteristics of waxy crude treated by PPD have been investigated. The conclusions are as follows: PPD can reduce the pour point and abnormal point of waxy crude, broaden the temperature range of Newtonian fluid of waxy crude, and lower greatly the viscosity of non-Newtonian fluid of waxy crude. The influence of reheating and high-rate shear on the effect of PPD mainly depends on their temperature. When the reheating temperature is more than the abnormal point of crude by 10℃, the reheating process has little effect on the modification effect of PPD. However, when the reheating temperature is below the abnormal point of crude, the reheating process will reduce the modification effect of PPD. When temperature is above the abnormal point of crude, the high-rate shear has little effect on the modification effect of PPD. At a temperature range where a lot of wax is precipitating, high-rate shear will greatly reduce the modification effect of PPD.展开更多
In order to clarify the characteristics and formation mechanism of the reheat cracking in Ti2AlNb weldments,a series of heat treatment conditions were performed to the circular joints welded by electron beam,and then ...In order to clarify the characteristics and formation mechanism of the reheat cracking in Ti2AlNb weldments,a series of heat treatment conditions were performed to the circular joints welded by electron beam,and then the macrostructures and microstructures were investigated using optical microscopy,scanning electron microscopy,X-ray diffractometry,and transmission electron microscopy.The results show that the reheat cracking occurs primarily along the grain boundaries in the weld when the Ti2AlNb circular welded joints are heated up to about 700℃.During the heat treatment,an almost complete transformation of B2→O happens while the temperature goes up through the O single-phase region.Then,O→B2+O phase transformation occurs primarily along the grain boundaries as the weld metal continues to heat up to the B2+O dual-phase region.Under the high tension stress consisting of welding residual stress and phase transformation stress,reheat cracking occurs at the interface between the B2+O dual-phase layer and the O-phase matrix.展开更多
文摘Pour point depressants (PPD) are used to improve the theology of waxy crude. The affect of various factors on the theological properties, and the thermal characteristics of waxy crude treated by PPD have been investigated. The conclusions are as follows: PPD can reduce the pour point and abnormal point of waxy crude, broaden the temperature range of Newtonian fluid of waxy crude, and lower greatly the viscosity of non-Newtonian fluid of waxy crude. The influence of reheating and high-rate shear on the effect of PPD mainly depends on their temperature. When the reheating temperature is more than the abnormal point of crude by 10℃, the reheating process has little effect on the modification effect of PPD. However, when the reheating temperature is below the abnormal point of crude, the reheating process will reduce the modification effect of PPD. When temperature is above the abnormal point of crude, the high-rate shear has little effect on the modification effect of PPD. At a temperature range where a lot of wax is precipitating, high-rate shear will greatly reduce the modification effect of PPD.
文摘In order to clarify the characteristics and formation mechanism of the reheat cracking in Ti2AlNb weldments,a series of heat treatment conditions were performed to the circular joints welded by electron beam,and then the macrostructures and microstructures were investigated using optical microscopy,scanning electron microscopy,X-ray diffractometry,and transmission electron microscopy.The results show that the reheat cracking occurs primarily along the grain boundaries in the weld when the Ti2AlNb circular welded joints are heated up to about 700℃.During the heat treatment,an almost complete transformation of B2→O happens while the temperature goes up through the O single-phase region.Then,O→B2+O phase transformation occurs primarily along the grain boundaries as the weld metal continues to heat up to the B2+O dual-phase region.Under the high tension stress consisting of welding residual stress and phase transformation stress,reheat cracking occurs at the interface between the B2+O dual-phase layer and the O-phase matrix.