聚丁二酸-己二酸丁二醇酯的合成与表征 被引量:5
1
作者 黄辰昊 宋力 +1 位作者 苏婷婷 王战勇 《中国塑料》 CAS CSCD 北大核心 2023年第5期34-39,共6页
以1,4-丁二醇及不同比例的己二酸、丁二酸为原料,制备一系列聚丁二酸-己二酸丁二醇酯[P(BS-co-BA)]共聚酯,借助衰减全反射傅里叶变换红外光谱仪(ATR-FTIR)、核磁共振仪(1H-NMR)、差示扫描量热仪(DSC)、X射线衍射仪(XRD)以及热重分析仪(... 以1,4-丁二醇及不同比例的己二酸、丁二酸为原料,制备一系列聚丁二酸-己二酸丁二醇酯[P(BS-co-BA)]共聚酯,借助衰减全反射傅里叶变换红外光谱仪(ATR-FTIR)、核磁共振仪(1H-NMR)、差示扫描量热仪(DSC)、X射线衍射仪(XRD)以及热重分析仪(TG)等对共聚酯的结构性能进行表征分析。角质酶降解结果表明,在经过16 h后,4种共聚酯降解率均达到80%以上,2种均聚酯均仅为40%左右。其中聚酯酶降解速率为P(BS-co-40%BA)>P(BS-co-60%BA)>P(BS-co-80%BA)>P(BS-co-20%BA)>聚己二酸丁二醇酯(PBA)>聚丁二酸丁二醇酯(PBS)。综合可知P(BS-co-40%BA)热稳定性相比于PBA更好,降解性能较PBS更好,为最佳共聚酯。 展开更多
关键词 共聚酯 聚丁二酸丁二醇酯 聚己二酸丁二醇酯 酶降解
下载PDF
Effects of Crystallization Temperature and Blend Ratio on the Crystal Structure of Poly(butylene adipate) in the Poly(butylene adipate)/Poly(butylene succinate) Blends 被引量:3
2
作者 Hai-jun Wang Hui-ping Feng +6 位作者 王学川 Pei-ying Guo Ting-shan Zhao Long-fang Ren Xi-huai Qiang Yu-hao Xiang 晏超 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2014年第4期488-496,共9页
The effects of crystallization temperature and blend ratio on the polymorphic crystal structures of poly(butylene adipate) (PBA) in poly(butylene succinate) (PBS)/poly(butylene adipate) (PBS/PBA) blends we... The effects of crystallization temperature and blend ratio on the polymorphic crystal structures of poly(butylene adipate) (PBA) in poly(butylene succinate) (PBS)/poly(butylene adipate) (PBS/PBA) blends were studied by means of differential scanning calorimetry (DSC), wide-angle X-ray diffraction (XRD) and atomic force microscopy (AFM). It was revealed that the polymorphism of PBA can be regulated by the blend ratio even in a non-isothermal crystallization process. The results demonstrate that high temperature favors fiat-on α crystals, while low temperature contributes to edge-on β crystals. It was also found that the effect of blend ratio on the crystallization mechanism of PBA is well coincident with that of the crystallization temperature. The increment of PBS content in the PBS/PBA blend gives rise to more β-form crystals of PBA. For those PBS/PBA blends with low PBA content, the interlamellar phase segregation of PBA makes its molecular chains so difficult to diffuse from one isolated microdomain to another that high crystallization temperature and sufficiently long crystallization time will be required if the PBA α-type crystals are targeted. 展开更多
关键词 BLENDS CRYSTALLIZATION polybutylene adipate polybutylene succinate).
原文传递
聚酯纤维的附生结晶法改善纤维的表面浸润性 被引量:5
3
作者 王海军 赵庭山 +3 位作者 石宝 任龙芳 强涛涛 王学川 《高分子材料科学与工程》 EI CAS CSCD 北大核心 2012年第10期39-42,共4页
将聚对苯二甲酸乙二醇酯(PET)纤维置入过冷态的聚乙二醇(PEG)和聚己二酸丁二酯(PBA)熔体,制备了PET纤维/PEG基体和PET纤维/PBA基体复合体系。使用偏光显微镜和原子力显微镜研究了这两种异质复合体系的界面结晶形态,利用接触角测量仪测... 将聚对苯二甲酸乙二醇酯(PET)纤维置入过冷态的聚乙二醇(PEG)和聚己二酸丁二酯(PBA)熔体,制备了PET纤维/PEG基体和PET纤维/PBA基体复合体系。使用偏光显微镜和原子力显微镜研究了这两种异质复合体系的界面结晶形态,利用接触角测量仪测量了附生结晶法改性前后PET纤维织物的接触角。结果表明,纤维置入温度和结晶等条件决定附生体系的横穿晶体形态结构,选取合适的树脂并采用附生结晶的方法可明显改善PET纤维织物的表面浸润性,并有望改善PET纤维增强复合材料内部的界面结构。 展开更多
关键词 附生结晶 聚酯纤维 聚乙二醇 聚己二酸丁二酯
下载PDF
聚己二酸丁二醇酯的制备与表征
4
作者 杨代兰 杨震 +3 位作者 李梓媛 袁明龙 李袁帅 袁明伟 《塑料工业》 CAS CSCD 北大核心 2024年第3期34-40,共7页
在180~200℃、质量分数为0.2%的钛酸四丁酯催化剂的条件下,1,6-己二酸和1,4-丁二醇(酸/醇物质的量比为1∶1.05、1∶1.10、1∶1.15、1∶1.20、1∶1.25)通过酯化、缩聚合成以羟基封端的、生物降解的聚己二酸丁二醇酯(PBA),同时比较不同酸... 在180~200℃、质量分数为0.2%的钛酸四丁酯催化剂的条件下,1,6-己二酸和1,4-丁二醇(酸/醇物质的量比为1∶1.05、1∶1.10、1∶1.15、1∶1.20、1∶1.25)通过酯化、缩聚合成以羟基封端的、生物降解的聚己二酸丁二醇酯(PBA),同时比较不同酸/醇物质的量比合成的PBA性能,筛选出合成PBA的最佳酸/醇物质的量比。结果表明,酸/醇物质的量比为1∶1.05时,PBA的分子量(31884)最高,产物具有一定的韧性、更优异的拉伸性能和较高的薄膜平整度,拉伸强度为15.81 MPa,断裂伸长率高达824.62%;5个酸/醇物质的量比条件下制备的PBA的热分解温度均在350℃以上,产物具有较好的热稳定性。该合成方法的装置简单、聚合时间相对较短,且实验条件易于实现。 展开更多
关键词 聚己二酸丁二醇酯 生物降解 脂肪族聚酯 热稳定性 拉伸性能
下载PDF
支化聚己二酸丁二醇酯的制备及其对PVC增塑作用的研究 被引量:5
5
作者 符金玉 赵岩岩 +1 位作者 李艳 谢吉星 《中国塑料》 CSCD 北大核心 2017年第8期100-104,共5页
以丙三醇为支化剂,己二酸和1,4-丁二醇为原料,通过酯化缩聚法合成出一系列具有不同特性黏度的支化聚己二酸丁二醇酯(BPBA),并将BPBA作为增塑剂应用在聚氯乙烯(PVC)中,与4种传统增塑剂邻苯二甲酸二辛酯(DOP)、线形聚己二酸丁二醇酯(LPBA... 以丙三醇为支化剂,己二酸和1,4-丁二醇为原料,通过酯化缩聚法合成出一系列具有不同特性黏度的支化聚己二酸丁二醇酯(BPBA),并将BPBA作为增塑剂应用在聚氯乙烯(PVC)中,与4种传统增塑剂邻苯二甲酸二辛酯(DOP)、线形聚己二酸丁二醇酯(LPBA)和环氧大豆油(ESBO)、乙酰柠檬酸三丁酯(ATBC)分别进行了性能对比。结果表明,当支化剂含量为0.5%(物质的量百分比),反应时间为5h时,BPBA的特性黏度最小为0.105dL/g;当BPBA含量为0.5%时,PVC/BPBA样品的断裂伸长率比PVC/LPBA和PVC/ESBO分别提高了22.4%和14.6%,低温韧性分别提高了15.7%和34.8%;BPBA相比于DOP、ATBC具有更好的热稳定性和耐迁出性。 展开更多
关键词 聚己二酸丁二醇酯 聚氯乙烯 支化 增塑剂 迁出性
下载PDF
热处理对聚己二酸丁二酯多晶结构和降解行为的影响 被引量:5
6
作者 赵丽芬 蒋妮 甘志华 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2011年第1期185-189,共5页
通过熔融结晶并结合退火处理方法得到多晶结构的聚己二酸丁二酯(PBA)及具有不同热历史的热力学稳定的α晶型,采用广角X射线衍射仪(WAXD)、原子力显微镜(AFM)和差示扫描量热仪(DSC)研究了PBA的多晶结构、晶体尺寸和结晶形貌,跟踪了退火处... 通过熔融结晶并结合退火处理方法得到多晶结构的聚己二酸丁二酯(PBA)及具有不同热历史的热力学稳定的α晶型,采用广角X射线衍射仪(WAXD)、原子力显微镜(AFM)和差示扫描量热仪(DSC)研究了PBA的多晶结构、晶体尺寸和结晶形貌,跟踪了退火处理PBA的生物降解行为.结果表明,分子链在相同晶格排列中围绕c轴空间取向的不同是决定多晶PBA降解速率差别的根本因素. 展开更多
关键词 聚己二酸丁二醇酯 多晶结构 退火处理 生物降解
下载PDF
聚偏氟乙烯/聚己二酸丁二醇酯复合薄膜的晶体结构与性能 被引量:3
7
作者 王海军 阮潇潇 《高分子材料科学与工程》 EI CAS CSCD 北大核心 2018年第4期49-53,共5页
采用溶液共混法制备聚偏氟乙烯/聚己二酸丁二醇酯(PVDF/PBA)复合薄膜,通过偏光显微镜、扫描电子显微镜、差示扫描量热仪和傅里叶变换红外光谱研究了复合体系在不同的共混比例的形貌和晶体结构变化,通过TF Analyzer2000分析了PBA组分的... 采用溶液共混法制备聚偏氟乙烯/聚己二酸丁二醇酯(PVDF/PBA)复合薄膜,通过偏光显微镜、扫描电子显微镜、差示扫描量热仪和傅里叶变换红外光谱研究了复合体系在不同的共混比例的形貌和晶体结构变化,通过TF Analyzer2000分析了PBA组分的加入对复合体系电性能的影响。结果表明:α型PVDF环带球晶的环带间距随着体系内PBA含量的增多而增大,并且同一球晶外延的环带间距大于球晶中心位置的环带间距;PBA的加入促进了γ-PVDF晶体的生成,PVDF/PBA复合材料具有较高的矫顽场和剩余极化强度。 展开更多
关键词 聚偏氟乙烯 聚己二酸丁二醇酯 晶体结构
下载PDF
Influence of Teflon Substrate on Crystallization and Enzymatic Degradation of Polymorphic Poly(butylene adipate) 被引量:1
8
作者 Zhen-bo Ning Ronnie Nielsen +2 位作者 Li-fen Zhao Dong-hong Yu 甘志华 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2014年第9期1243-1252,共10页
Oriented and non-oriented Teflon films, which were found to have the same crystalline structure, but different surface morphologies, were used to sandwich poly(butylene adipate) (PBA) films during isothermal cryst... Oriented and non-oriented Teflon films, which were found to have the same crystalline structure, but different surface morphologies, were used to sandwich poly(butylene adipate) (PBA) films during isothermal crystallization. It was found that both the Teflon surface structure and the PBA polymorphic structure are the determining factors to induce epitaxial crystallization. The oriented Teflon film was able to induce epitaxial crystallization of PBA α crystal, while the non-oriented Teflon did not induce any epitaxial crystallization of PBA. Epitaxial crystallization did not occurred for PBA β crystals between neither the oriented nor the non-oriented Teflon films. The enzymatic degradation rate of PBA films was not determined by the epitaxial crystallization, in fact it was still dependent on the polymorphic crystal structure of PBA. The morphological changes of PBA films after enzymatic degradation confirmed again that the epitaxial crystallization only occurred for the PBA film with α crystal structure which was produced by being sandwiched between oriented Teflon films, and it happened only on the surface of PBA films. 展开更多
关键词 polybutylene adipate Epitaxial crystallization polymorphic crystals Enzymatic degradation Morphology.
原文传递
溶液与熔融相结合合成脂肪族聚酯
9
作者 张昌辉 翟文举 +1 位作者 赵霞 寇莹 《塑料》 CAS CSCD 北大核心 2009年第4期61-63,91,共4页
采用溶液与熔融结合法合成了聚丁二酸丁二醇酯(PBS)、聚己二酸丁二醇酯(PBA)、聚癸二酸丁二醇酯(PBSe)。采用1H NMR对聚合物结构进行表征,采用凝胶渗透色谱、热重分析和万能实验机测定PBS的相对分子质量及分布、热稳定性和力学性能。实... 采用溶液与熔融结合法合成了聚丁二酸丁二醇酯(PBS)、聚己二酸丁二醇酯(PBA)、聚癸二酸丁二醇酯(PBSe)。采用1H NMR对聚合物结构进行表征,采用凝胶渗透色谱、热重分析和万能实验机测定PBS的相对分子质量及分布、热稳定性和力学性能。实验结果表明:聚酯的数均分子量都在5万以上,热分解起始温度均在300℃以上,断裂伸长率都大于300%,其中PBA更是超过了400%;结构对称性是熔点和生物降解性的主要影响因素,碳链的长短是热分解的主要影响因素。 展开更多
关键词 脂肪族聚酯 生物降解性 聚丁二酸丁二醇酯 聚己二酸丁二醇酯 聚癸二酸丁二醇酯
下载PDF
Thermal Behavior and Crystal Transition of Biodegradable Poly(butylenes adipate)Revealed by Two-Dimensional Correlation Spectroscopy
10
作者 CHEN Yu-jing Isao Noda Young Mee Jung 《光谱学与光谱分析》 SCIE EI CAS CSCD 北大核心 2016年第S1期139-140,共2页
In the present study,thermal behavior and crystal transition of pure poly(butylene adipate)(PBA)upon heating process were investigated by FTIR spectroscopy.To gain further insight into the thermal behavior alteration ... In the present study,thermal behavior and crystal transition of pure poly(butylene adipate)(PBA)upon heating process were investigated by FTIR spectroscopy.To gain further insight into the thermal behavior alteration and the phase transition of PBA,we performed two-dimensional(2D)correlation analysis.We found thatβ-form PBA crystal undergoes not only the melting process but also crystal transition upon the heating process. 展开更多
关键词 poly(butylene adipate) Thermal behavior Crystal transition Two-dimensional correlation spec-troscopy
下载PDF
Prominently Promoting the Formation of Poly(butylene adipate) α-Form Crystals by Coalescing from Inclusion Complex
11
作者 Hai-Mu Ye Xiao-Tong Chen +1 位作者 Ping Liu Na Yan 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2018年第7期866-870,共5页
We successfully use a co-precipitation method to prepare inclusion complex between poly(butylene adipate) (PBA) chains (guest component) and urea molecules (host component). The PBA/urea inclusion complex is c... We successfully use a co-precipitation method to prepare inclusion complex between poly(butylene adipate) (PBA) chains (guest component) and urea molecules (host component). The PBA/urea inclusion complex is confirmed to adopt a hexagonal crystal modification with lattice parameters ofa = 8.14 A and c = 10.92 A, and the interaction between PBA chains and urea is van der Waals force. The singly isolated PBA chains are suggested to take some gauche conformation, which is different from the all-trans conformation in r-form PBA. Furthermore, we employ the isolated PBA chains which are uniformly pre-established in a specific conformation in urea channels to regulate the crystal form of PBA for the first time. After removing the host urea molecules, the coalesced PBA chains are found to solely crystallize into a-form crystals at different coalescing temperatures. By comparing the FTIR spectra, it is found that PBA chains in inclusion complex plausibly contain some similar conformers as those in a-form crystal, which is suggested to be the intrinsic reason for the sole formation of a-form crystals. This research proves that inclusion complex can be used as a very effective method to regulate polymorphism of semi-crystalline polymers. 展开更多
关键词 polybutylene adipate Inclusion complex polyMORPHISM Chain conformation
原文传递
剪切诱导聚己二酸丁二醇酯的结晶行为 被引量:1
12
作者 王海军 李金祥 王学川 《高分子材料科学与工程》 EI CAS CSCD 北大核心 2014年第6期73-76,共4页
使用偏光显微镜、广角X射线衍射仪和扫描电子显微镜等测试手段,分别研究了纤维诱导和剪切作用下聚己二酸丁二醇酯(PBA)结晶的晶型结构和结晶形貌。结果表明,不同纤维置入过冷态PBA熔体时产生的剪切作用诱导PBA在纤维表面形成横晶结构。... 使用偏光显微镜、广角X射线衍射仪和扫描电子显微镜等测试手段,分别研究了纤维诱导和剪切作用下聚己二酸丁二醇酯(PBA)结晶的晶型结构和结晶形貌。结果表明,不同纤维置入过冷态PBA熔体时产生的剪切作用诱导PBA在纤维表面形成横晶结构。在剪切应力的作用下,PBA形成不同于球晶的高成核密度、高取向度的横晶。过冷度决定横晶的晶型结构,高温时形成热力学性能更为优异的α型横晶,而较低的结晶温度则有利于生成β型横晶。 展开更多
关键词 聚己二酸丁二醇酯 结晶 剪切
下载PDF
填料绢云母对聚己二酸丁二醇酯复合材料多晶结构的影响 被引量:1
13
作者 王海军 王帅毅 王学川 《高分子材料科学与工程》 EI CAS CSCD 北大核心 2017年第12期65-70,共6页
通过溶液浇铸法制备了聚己二酸丁二醇酯(PBA)/绢云母微粒复合材料。使用差示扫描量热、广角X射线衍射、偏光显微镜等手段研究了绢云母微粒/PBA复合材料中PBA结晶行为、多晶结构以及晶体形貌。结果表明,绢云母作为成核剂有效地增加PBA晶... 通过溶液浇铸法制备了聚己二酸丁二醇酯(PBA)/绢云母微粒复合材料。使用差示扫描量热、广角X射线衍射、偏光显微镜等手段研究了绢云母微粒/PBA复合材料中PBA结晶行为、多晶结构以及晶体形貌。结果表明,绢云母作为成核剂有效地增加PBA晶体成核密度、降低晶体尺寸。在较高的降温速率和较低的结晶温度下依然能生成稳定的α晶体,对比纯PBA在25℃的晶体类型,加入质量分数1%绢云母微粒后有生成α晶体结构存在。因此通过控制降温速率和添加绢云母微粒能够起到调控PBA多晶型结构。 展开更多
关键词 聚己二酸丁二醇酯 绢云母 复合材料 多晶结构
下载PDF
PES/PBA共混体系的相容性及其结晶行为
14
作者 王海军 冯会平 王学川 《青岛科技大学学报(自然科学版)》 CAS 2015年第4期413-417,共5页
采用溶液浇铸法制备了聚丁二酸乙二醇酯/聚己二酸丁二醇酯(PES/PBA)共混物,并使用偏光显微镜(POM)和差示扫描量热仪(DSC)等手段研究了PES/PBA共混物两种组分的相容性及结晶动力学。相分离形貌和玻璃化转变温度结果表明,PES/PBA共混物为... 采用溶液浇铸法制备了聚丁二酸乙二醇酯/聚己二酸丁二醇酯(PES/PBA)共混物,并使用偏光显微镜(POM)和差示扫描量热仪(DSC)等手段研究了PES/PBA共混物两种组分的相容性及结晶动力学。相分离形貌和玻璃化转变温度结果表明,PES/PBA共混物为热力学不相容共混体系。利用Avrami方程分别研究了共混物中两种组分的等温结晶动力学,并计算了相关的结晶动力学参数。PES的结晶速率随着PBA的增加而减小,Avrami指数基本不变;PBA的结晶速率也随着PBA含量的降低而减小,但其结晶机理不受共混比例的影响。 展开更多
关键词 聚丁二酸乙二醇酯(PES) 聚己二酸丁二醇酯(PBA) 共混 相容性 结晶
下载PDF
溴化钾对多晶型聚己二酸丁二醇酯结晶行为的调控作用
15
作者 王海军 阮潇潇 《青岛科技大学学报(自然科学版)》 CAS 2018年第3期36-41,共6页
使用偏光显微镜(POM)、差示扫描量热仪(DSC)和广角X射线衍射仪(WAXD)等测试手段,研究了PBA/KBr(聚己二酸丁二醇酯/溴化钾)复合材料中KBr对PBA结晶行为和晶体结构的影响规律。结果表明:随着KBr含量的增加,PBA的成核密度不断增大,而球晶... 使用偏光显微镜(POM)、差示扫描量热仪(DSC)和广角X射线衍射仪(WAXD)等测试手段,研究了PBA/KBr(聚己二酸丁二醇酯/溴化钾)复合材料中KBr对PBA结晶行为和晶体结构的影响规律。结果表明:随着KBr含量的增加,PBA的成核密度不断增大,而球晶尺寸不断减小。此外,PBA的结晶温度和结晶速率都随着KBr含量的增加而提高。WAXD和拉曼光谱研究进一步表明,KBr促进PBA生成热力学稳定且降解速率更快的α型晶体。 展开更多
关键词 聚己二酸丁二醇酯(PBA) 溴化钾(KBr) 复合材料 结晶
下载PDF
聚乳酸/PBAT共混物的制备及其性能研究 被引量:64
16
作者 顾书英 詹辉 任杰 《中国塑料》 CAS CSCD 北大核心 2006年第10期39-42,共4页
用熔融挤出法制备了聚乳酸/对苯二甲酸-己二酸-1,4-丁二醇三元共聚酯(PLA/PBAT)共混物,研究了聚乳酸/PBAT共混物的力学性能、热性能以及相容性。结果表明:共混物的冲击强度及断裂伸长率随着PBAT含量的增加而增大,在PBAT含量为30%时,... 用熔融挤出法制备了聚乳酸/对苯二甲酸-己二酸-1,4-丁二醇三元共聚酯(PLA/PBAT)共混物,研究了聚乳酸/PBAT共混物的力学性能、热性能以及相容性。结果表明:共混物的冲击强度及断裂伸长率随着PBAT含量的增加而增大,在PBAT含量为30%时,断裂伸长率最大,达到9%,PBAT的加入降低了共混物的拉伸、弯曲性能,但在添加量较少的情况下(如5%和10%),拉伸、弯曲性能下降不大。退火处理极大的提高了材料的维卡软化温度。当PBAT含量较高时,共混物的断面可以明显的观察到不相容的两相结构。 展开更多
关键词 聚乳酸 对苯二甲酸-己二酸-1 4-丁二醇三元共聚酯 力学性能 相容性
下载PDF
聚己二酸对苯二甲酸丁二酯(PBAT)共混改性聚乳酸(PLA)高性能全生物降解复合材料研究进展 被引量:36
17
作者 王鑫 石敏 +2 位作者 余晓磊 彭少贤 赵西坡 《材料导报》 EI CAS CSCD 北大核心 2019年第11期1897-1909,共13页
聚乳酸(PLA)作为一种可降解、可再生的聚合物,其优异的生物相容性和高强度、高模量的力学性能引起了许多学者的关注。聚乳酸基生物复合材料自进入人们的视野以来,由于其固有的延展性差、冲击强度低,加工过程结晶速率慢,结晶度小等缺陷,... 聚乳酸(PLA)作为一种可降解、可再生的聚合物,其优异的生物相容性和高强度、高模量的力学性能引起了许多学者的关注。聚乳酸基生物复合材料自进入人们的视野以来,由于其固有的延展性差、冲击强度低,加工过程结晶速率慢,结晶度小等缺陷,严重阻碍了其发展。关于PLA的改性研究在近十年里从未间断过,主要集中在增塑改性、增强改性、增韧改性。增塑改性是指向PLA中加入乳酸低聚物、柠檬酸酯、聚乙二醇等小分子化合物,减少PLA分子链间的相互作用,改善PLA的塑性,断裂伸长率大幅度提高,但增塑剂易渗出、迁移是如今面临的一大难题;增强改性是指向PLA加入无机填料或纳米粒子(二氧化硅(SiO 2)、二氧化钛(TiO 2)、碳酸钙(CaCO 3)、滑石粉(Talc)、蒙脱土(MMT)等)引发异相成核,改善PLA的结晶性能,但无法从根本上解决材料韧性差的缺陷;增韧改性是指加入橡胶粒子或热塑性弹性体(天然橡胶(NR)、热塑性聚氨酯(TPU)、聚碳酸酯(PC)等),虽然在一定程度上改善了PLA的韧性,但PLA的生物降解性无法保证;随着一些可降解聚酯(聚己内酯(PCL)、聚丁二酸丁二醇酯(PBS)、聚己二酸对苯二甲酸丁二酯(PBAT)等)的产生,在不改变降解性能下,对PLA进行有效的增韧改性,是聚乳酸改性研究的主要方向和研究热点。PBAT作为一种可降解聚酯聚合物,链段兼具长链脂肪烃的柔性和芳环的刚性,赋予了其优异的柔韧性,与其他聚酯材料相比,这一优势是作为增韧改性PLA的最佳选择。在早期PLA/PBAT的研究过程中就发现,由于分子链段上结构的巨大差异,PBAT与PLA的相容性差导致共混物力学性能不佳。近十年里,研究者在聚合物共混改性的基础上,选择合适的第三组分对PLA/PBAT共混体系进行改性,并取得了丰硕的成果。目前,PLA/PBAT共混体系的增韧后冲击强度由纯PLA的2.3 kJ/m 2提高至61.9 kJ/m 2。本文归纳了PB 展开更多
关键词 聚乳酸 聚己二酸对苯二甲酸丁二酯 生物降解 反应性共混
下载PDF
PBS/PBAT共混型全生物降解材料的制备及其性能研究 被引量:27
18
作者 吕怀兴 杨彪 许国志 《中国塑料》 CAS CSCD 北大核心 2009年第8期18-21,共4页
通过熔融共混法制备了聚丁二酸丁二醇酯(PBS)/聚己二酸对苯二甲酸丁二酯(PBAT)共混物,用熔体流动速率仪、差示扫描量热仪、X射线衍射仪、扫描电镜及力学性能测试等手段研究了PBS/PBAT共混物的熔体流动性、结晶性能、力学性能以及共混物... 通过熔融共混法制备了聚丁二酸丁二醇酯(PBS)/聚己二酸对苯二甲酸丁二酯(PBAT)共混物,用熔体流动速率仪、差示扫描量热仪、X射线衍射仪、扫描电镜及力学性能测试等手段研究了PBS/PBAT共混物的熔体流动性、结晶性能、力学性能以及共混物相容性。结果表明,随着PBAT含量的增加,PBS/PBAT共混体系的拉伸强度先升高后降低,断裂伸长率不断提高,冲击强度先降低后提高;当PBAT含量为20%(质量分数,下同)时,与纯PBS相比,断裂伸长率提高了10倍,冲击强度提高了82%,而拉伸强度仅降低6%。 展开更多
关键词 全生物降解塑料 聚丁二烯丁二醇酯 聚己二酸对苯二甲酸丁二酯 结晶 性能
下载PDF
可生物降解塑料PBAT共混改性研究进展 被引量:27
19
作者 晏永祥 贺哲 +2 位作者 张跃飞 李焰 申雄军 《工程塑料应用》 CAS CSCD 北大核心 2021年第5期158-161,共4页
可生物降解塑料聚己二酸对苯二甲酸丁二酯(PBAT)的改性是降低其成本、提高性能的重要方法。主要综述了近十几年来国内外PBAT的共混改性研究进展,主要包括聚乳酸、聚碳酸亚丙酯、聚丁二酸丁二醇酯、聚羟基丁酸戊酯、聚乙醇酸、聚乙烯醇... 可生物降解塑料聚己二酸对苯二甲酸丁二酯(PBAT)的改性是降低其成本、提高性能的重要方法。主要综述了近十几年来国内外PBAT的共混改性研究进展,主要包括聚乳酸、聚碳酸亚丙酯、聚丁二酸丁二醇酯、聚羟基丁酸戊酯、聚乙醇酸、聚乙烯醇缩丁醛等可降解高分子与PBAT共混改性,玉米淀粉、纤维素和木质素等有机填料与PBAT共混改性,以及碳酸钙、蒙脱土等无机填料与PBAT共混改性,并对其发展作出总结与展望,旨在为开发新型高效的PBAT复合材料提供指导意义。 展开更多
关键词 聚己二酸对苯二甲酸丁二酯 可降解高分子聚合物 填料 共混改性
下载PDF
PBAT合成工艺研究 被引量:25
20
作者 庞道双 潘小虎 +1 位作者 李乃祥 戴钧明 《合成技术及应用》 2019年第2期35-39,共5页
以己二酸(AA)、对苯二甲酸(PTA)、丁二醇(BDO)为单体,合成了聚己二酸丁二醇-co-对苯二甲酸丁二醇酯(PBAT),考察了酯化方式、酯化时间、缩聚温度、稳定剂等关键工艺对合成过程及产品性能的影响,确定了制备良好色相PBAT树脂的工艺条件:共... 以己二酸(AA)、对苯二甲酸(PTA)、丁二醇(BDO)为单体,合成了聚己二酸丁二醇-co-对苯二甲酸丁二醇酯(PBAT),考察了酯化方式、酯化时间、缩聚温度、稳定剂等关键工艺对合成过程及产品性能的影响,确定了制备良好色相PBAT树脂的工艺条件:共酯化方式,酯化时间185min,缩聚温度248~250℃,稳定剂添加量70μg/g。对AA理论加入量与实测值差异分析发现:己二酸以2~3个聚合度的己二酸低聚物形式通过真空系统抽出,可以再聚合使用。 展开更多