Arsenic is selectively extracted from high-arsenic dust by NaOH-Na2S alkaline leaching process. In the leaching arsenic process, the effects of alkali-to-dust ratio, sodium sulfide addition, leaching temperature, leac...Arsenic is selectively extracted from high-arsenic dust by NaOH-Na2S alkaline leaching process. In the leaching arsenic process, the effects of alkali-to-dust ratio, sodium sulfide addition, leaching temperature, leaching time and liquid-to-solid ratio on metals leaching efficiencies were investigated. The results show that the arsenic can be effectively separated from other metals under the optimum conditions of alkali/dust mass ratio of 0.5, sodium sulfide addition of 0.25 g/g, leaching temperature of 90 ℃, leaching time of 2 h, and liquid-to-solid ratio of 5:1 (mL/g). Under these conditions, the average leaching efficiencies of arsenic, antimony, lead, tin and zinc are 92.75%, 11.68%, 0.31%, 29.75% and 36.85%, respectively. The NaOH-Na2S alkaline leaching process provides a simple and highly efficient way to remove arsenic from high-arsenic dust, leaving residue as a suitable lead resource.展开更多
Two acidic ferrisols, i.e., red soil (RS) and yellow red soil (YRS), from the vicinity regions of non-ferrous ores in Hunan province of China, were leached with simulated acid rain through artificial column experi...Two acidic ferrisols, i.e., red soil (RS) and yellow red soil (YRS), from the vicinity regions of non-ferrous ores in Hunan province of China, were leached with simulated acid rain through artificial column experiments. The results show that the total leaching mass of metals are m(Zn)〉m(Cu)〉m(Cd) from the original soils and m(Cd)〉m(Zn)〉〉 m(Cu) from the contaminated soils with external metals after leaching for 60 d continuously, leaching quantities of Cd and Zn from the contaminated red soil (CRS) are more than that from the contaminated yellow red soil (CYRS), but for Cu, it is almost the same. The preferential fractions for leaching are mainly in exchangeable forms, and content of exchangeable forms decreases significantly in the contaminated soil profiles. The unstable fractions of Cd, Cu and Zn in the RS and YRS increase significantly with the decrease of pH value of simulated acid rain. Changes of fi, actions of external Cd, Cu, and Zn in the residual CRS and CYRS profiles are significantly affected by the acidity of acid rain, too. After leaching for 60 d continuously, Cd exists mostly in exchangeable form, Cu exists mainly in exchangeable, manganese oxide-occluded and organically bounding forms, and Zn exists in residual in CRS and CYRS profiles. Most of exchangeable Cd and Zn exist only small in surface layer (0-20 cm) and are transferred to the sub-layers, contrarily, Cu accumulates mostly in the topsoil (0-20 cm) with low translocation.展开更多
The leaching behavior of metals from a nickeliferous limonitic laterite ore was investigated by high pressure acid leaching process for the extraction of nickel and cobalt.The effects of sulfuric acid added,leaching t...The leaching behavior of metals from a nickeliferous limonitic laterite ore was investigated by high pressure acid leaching process for the extraction of nickel and cobalt.The effects of sulfuric acid added,leaching temperature,leaching time and liquid/solid(L/S) ratio on metals extraction were examined.More than 97% Ni,96% Co,93% Mn,95% Mg and less than 1% Fe are extracted under optimum conditions.Analysis of the high pressure acid leaching residue by chemical and XRD analysis indicates that the residual iron and sulfur are mainly present in phases of hematite and alunite,respectively.The high pressure leaching process provides a simple and efficient way for the high recovery of nickel and cobalt from laterite ore,leaving residue as a suitable iron resource.展开更多
Phosphogypsum(PG)is a typical by-product of phosphoric acid and phosphate fertilizers during acid digestion.The application of cemented paste backfill(CPB)has been feasibly investigated for the remediation of PG.The p...Phosphogypsum(PG)is a typical by-product of phosphoric acid and phosphate fertilizers during acid digestion.The application of cemented paste backfill(CPB)has been feasibly investigated for the remediation of PG.The present study evaluated fluorine immobilization mechanisms and attempted to construct a related thermodynamic and geochemical modeling to describe the related stabilization performance.Physico-chemical and mineralogical analyses were performed on PG and hardened PG-based CPB(PCPB).The correlated macro-and micro-structural properties were obtained from the analysis of the combination of unconfined compressive strength and scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy imaging.Acid/base-dependent leaching tests were performed to ascertain fluoride leachab-ility.In addition,Gibbs Energy Minimization Software and PHREEQC were applied as tools to characterize the PCPB hydration and deduce its geochemical characteristics.The results proved that multiple factors are involved in fluorine stabilization,among which the calcium silicate hy-drate gel was found to be associated with retention.Although the quantitative comparison with the experimental data shows that further modi-fication should be introduced into the simulation before being used as a predictive implement to determine PG management options,the im-portance of acid/base concentration in regulating the leaching behavior was confirmed.Moreover,the modeling enabled the identification of the impurity phases controlling the stability and leachability.展开更多
This paper investigates the leaching behavior of heavy metals(V,Pb,Cd,Cr,and As) from stone coal waste rocks with various particle sizes using dynamic leaching experiments.The results show that the dissolved concentra...This paper investigates the leaching behavior of heavy metals(V,Pb,Cd,Cr,and As) from stone coal waste rocks with various particle sizes using dynamic leaching experiments.The results show that the dissolved concentrations of V and As initially increased and then slightly decreased as time progressed and that the dissolved concentrations of Pb,Cd,and Cr were high in the early stage before decreasing.The particle size of the stone coal waste rocks strongly influenced the heavy metal concentration in the leaching solutions.The effects of the particle size of the stone coal waste rocks on the dissolved concentrations of V,Pb,and As decreased in the order fine fraction > medium fraction > coarse fraction,and the effects of particle size on the dissolved concentrations of Cr and Cd decreased in the order medium fraction > coarse fraction > fine fraction and coarse fraction > medium fraction > fine fraction,respectively.The quantities of heavy metals dissolved from the stone coal waste rock with fine particle sizes were observed to decrease in the order V(17104.36 μg/kg) > As(609.41 μg/kg) > Pb(469.24 μg/kg) > Cr(56.35 μg/kg) > Cd(27.52 μg/kg),and the dissolution rates decreased in the order As(2.96%) > Pb(0.93%) > V(0.35%) > Cd(0.25%) > Cr(0.01%).The specific surface area,pore size of the stone coal waste rocks,and chemical forms of heavy metals also influenced the release of heavy metals from the stone coal waste rocks.Kinetic analysis showed that the dissolution of heavy metals fundamentally agreed with the rate equation controlled by the shrinking core model.The results of this study are expected to serve as a reference for the evaluation of heavy metals contamination from stone coal waste rocks.展开更多
This study focused on leaching behavior of alkaline anion and sodium in bauxite residue through ammonium chloride treatment.The results showed that the pH of bauxite residue decreased from 10.49 to 8.93,total alkaline...This study focused on leaching behavior of alkaline anion and sodium in bauxite residue through ammonium chloride treatment.The results showed that the pH of bauxite residue decreased from 10.49 to 8.93,total alkaline anion(HCO3^-,CO3^2-,OH^-,AlO2^-)concentration reduced from 38.89 to 25.50 mmol/L,leaching rate of soluble sodium was 80.86%with ammonium chloride addition of 0.75%,liquid/solid(L/S)ratio of 3(mL/g),temperature of 30°C and reaction time of 18 h;L/S ratio was the main factor affecting the removal of alkaline anion and the leaching of sodium.Furthermore,ammonium chloride promoted the dissolution of diaspore and changed the micro/morphological characteristics with the increase of massive structure.The findings of this work will contribute to achieve soil-formation of bauxite residue.展开更多
Physicochemical properties and leaching behaviors of two typical arsenic-bearing lime?ferrate sludges(ABLFS),waste acid residue(WAR)and calcium arsenate residue(CAR),are comprehensively described.The chemical composit...Physicochemical properties and leaching behaviors of two typical arsenic-bearing lime?ferrate sludges(ABLFS),waste acid residue(WAR)and calcium arsenate residue(CAR),are comprehensively described.The chemical composition,morphological features,phase composition and arsenic occurrence state of WAR and CAR are analyzed by ICP?AES,SEM?EDS,XRD,XPS and chemical phase analysis.The toxicity leaching test and three-stage BCR sequential extraction procedure are utilized to investigate arsenic leaching behaviors.The results show that the contents of arsenic in WAR and CAR are2.5%and21.2%and mainly present in the phases of arsenate and arsenic oxides dispersed uniformly or agglomerated in amorphous particles.The leaching concentrations of arsenic excess119and1063times of TCLP standard regulatory level with leaching rates of47.66%and50.15%for WAR and CAR,respectively.About90%of extracted arsenic is in the form of acid soluble and reducible,which is the reason of high arsenic leaching toxicity and environmental activity of ABLFS.This research provides comprehensive information on harmless disposal of ABLFS from industrial wastewater treatment of lime?ferrate process.展开更多
Bauxite residue is a highly alkaline waste containing soluble alkaline anions, which can cause environmental concerns. The optimal leaching conditions, distribution of alkaline anions, types of pivotal alkaline anions...Bauxite residue is a highly alkaline waste containing soluble alkaline anions, which can cause environmental concerns. The optimal leaching conditions, distribution of alkaline anions, types of pivotal alkaline anions and their dissolution behaviors were investigated based on the combination of single factors-orthogonal experiments and leaching stage experiment. Using a two-stage leaching, 86% of the soluble alkaline anions(CO3^2-, HCO4^-,Al(OH)4^-, OH^-) were leached with a L/S ratio of 2 mL/g, at 30 ℃, over 23 h. During the first stage of leaching, approximately 88% of alkaline anions were leached from the dissolution of free alkali(Na OH, carbonate, bicarbonate, NaAl(OH)4) with the rest originating from the dissolution of alkaline minerals(calcite, cancrinite and hydrogarnet). Supernatant alkalinity was 69.78 mmol/L with CO3^2- accounting for 75%. Furthermore, carbonate leaching was controlled by solid film diffusion using the Stumm Model with an apparent activation energy of 10.24 kJ/mol.展开更多
The leaching behavior of main metallic sulphides in zinc concentrate under atmospheric oxygen-rich direct leaching conditions was studied through mineralogical analysis. The results show that the sulphides dissolve ob...The leaching behavior of main metallic sulphides in zinc concentrate under atmospheric oxygen-rich direct leaching conditions was studied through mineralogical analysis. The results show that the sulphides dissolve obviously except pyrite. Based on the relationship between elemental sulfur and the residual sulphides in the leaching residue, the dissolution of sphalerite, chalcopyrite, covellite and galena is assumed to follow the indirect oxidation reactions, where the acidic dissolution takes place firstly and then the released H2S transfers from the mineral surface into bulk solution and is further oxidized into elemental sulfur. The interface chemical reaction is further supposed as the controlling step in the leaching of these sulphides. The direct electrochemical oxidation reactions are assumed to contribute to the dissolution of pyrrhotite, which is controlled by the diffusion through elemental sulfur layer.展开更多
基金Project(2012AA04022)supported by the Scientific Research and Technology Development Project of Guangxi,China
文摘Arsenic is selectively extracted from high-arsenic dust by NaOH-Na2S alkaline leaching process. In the leaching arsenic process, the effects of alkali-to-dust ratio, sodium sulfide addition, leaching temperature, leaching time and liquid-to-solid ratio on metals leaching efficiencies were investigated. The results show that the arsenic can be effectively separated from other metals under the optimum conditions of alkali/dust mass ratio of 0.5, sodium sulfide addition of 0.25 g/g, leaching temperature of 90 ℃, leaching time of 2 h, and liquid-to-solid ratio of 5:1 (mL/g). Under these conditions, the average leaching efficiencies of arsenic, antimony, lead, tin and zinc are 92.75%, 11.68%, 0.31%, 29.75% and 36.85%, respectively. The NaOH-Na2S alkaline leaching process provides a simple and highly efficient way to remove arsenic from high-arsenic dust, leaving residue as a suitable lead resource.
基金Project(20507022) supported by National Natural Science Foundation of China project(PRA E 00-04) supported by the Joint Research Fund for Chinese and French Scientists
文摘Two acidic ferrisols, i.e., red soil (RS) and yellow red soil (YRS), from the vicinity regions of non-ferrous ores in Hunan province of China, were leached with simulated acid rain through artificial column experiments. The results show that the total leaching mass of metals are m(Zn)〉m(Cu)〉m(Cd) from the original soils and m(Cd)〉m(Zn)〉〉 m(Cu) from the contaminated soils with external metals after leaching for 60 d continuously, leaching quantities of Cd and Zn from the contaminated red soil (CRS) are more than that from the contaminated yellow red soil (CYRS), but for Cu, it is almost the same. The preferential fractions for leaching are mainly in exchangeable forms, and content of exchangeable forms decreases significantly in the contaminated soil profiles. The unstable fractions of Cd, Cu and Zn in the RS and YRS increase significantly with the decrease of pH value of simulated acid rain. Changes of fi, actions of external Cd, Cu, and Zn in the residual CRS and CYRS profiles are significantly affected by the acidity of acid rain, too. After leaching for 60 d continuously, Cd exists mostly in exchangeable form, Cu exists mainly in exchangeable, manganese oxide-occluded and organically bounding forms, and Zn exists in residual in CRS and CYRS profiles. Most of exchangeable Cd and Zn exist only small in surface layer (0-20 cm) and are transferred to the sub-layers, contrarily, Cu accumulates mostly in the topsoil (0-20 cm) with low translocation.
文摘The leaching behavior of metals from a nickeliferous limonitic laterite ore was investigated by high pressure acid leaching process for the extraction of nickel and cobalt.The effects of sulfuric acid added,leaching temperature,leaching time and liquid/solid(L/S) ratio on metals extraction were examined.More than 97% Ni,96% Co,93% Mn,95% Mg and less than 1% Fe are extracted under optimum conditions.Analysis of the high pressure acid leaching residue by chemical and XRD analysis indicates that the residual iron and sulfur are mainly present in phases of hematite and alunite,respectively.The high pressure leaching process provides a simple and efficient way for the high recovery of nickel and cobalt from laterite ore,leaving residue as a suitable iron resource.
基金This work was financially supported by the Natural Science Foundation of Hunan Province,China(No.2020JJ5718)a scholarship granted by the China Scholarship Council(No.CSC201906370062)the National Natural Science Foundation of China(Nos.52004330 and 52074351).
文摘Phosphogypsum(PG)is a typical by-product of phosphoric acid and phosphate fertilizers during acid digestion.The application of cemented paste backfill(CPB)has been feasibly investigated for the remediation of PG.The present study evaluated fluorine immobilization mechanisms and attempted to construct a related thermodynamic and geochemical modeling to describe the related stabilization performance.Physico-chemical and mineralogical analyses were performed on PG and hardened PG-based CPB(PCPB).The correlated macro-and micro-structural properties were obtained from the analysis of the combination of unconfined compressive strength and scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy imaging.Acid/base-dependent leaching tests were performed to ascertain fluoride leachab-ility.In addition,Gibbs Energy Minimization Software and PHREEQC were applied as tools to characterize the PCPB hydration and deduce its geochemical characteristics.The results proved that multiple factors are involved in fluorine stabilization,among which the calcium silicate hy-drate gel was found to be associated with retention.Although the quantitative comparison with the experimental data shows that further modi-fication should be introduced into the simulation before being used as a predictive implement to determine PG management options,the im-portance of acid/base concentration in regulating the leaching behavior was confirmed.Moreover,the modeling enabled the identification of the impurity phases controlling the stability and leachability.
基金financially supported by the Major Science and Technology Program for Water Pollution Control and Treatment of China (No.2015ZX07205003)
文摘This paper investigates the leaching behavior of heavy metals(V,Pb,Cd,Cr,and As) from stone coal waste rocks with various particle sizes using dynamic leaching experiments.The results show that the dissolved concentrations of V and As initially increased and then slightly decreased as time progressed and that the dissolved concentrations of Pb,Cd,and Cr were high in the early stage before decreasing.The particle size of the stone coal waste rocks strongly influenced the heavy metal concentration in the leaching solutions.The effects of the particle size of the stone coal waste rocks on the dissolved concentrations of V,Pb,and As decreased in the order fine fraction > medium fraction > coarse fraction,and the effects of particle size on the dissolved concentrations of Cr and Cd decreased in the order medium fraction > coarse fraction > fine fraction and coarse fraction > medium fraction > fine fraction,respectively.The quantities of heavy metals dissolved from the stone coal waste rock with fine particle sizes were observed to decrease in the order V(17104.36 μg/kg) > As(609.41 μg/kg) > Pb(469.24 μg/kg) > Cr(56.35 μg/kg) > Cd(27.52 μg/kg),and the dissolution rates decreased in the order As(2.96%) > Pb(0.93%) > V(0.35%) > Cd(0.25%) > Cr(0.01%).The specific surface area,pore size of the stone coal waste rocks,and chemical forms of heavy metals also influenced the release of heavy metals from the stone coal waste rocks.Kinetic analysis showed that the dissolution of heavy metals fundamentally agreed with the rate equation controlled by the shrinking core model.The results of this study are expected to serve as a reference for the evaluation of heavy metals contamination from stone coal waste rocks.
基金Projects(41877511,41842020) supported by the National Natural Science Foundation of ChinaProject(201509048) supported by the Environmental Protection’s Special Scientific Research for Chinese Public Welfare Industry
文摘This study focused on leaching behavior of alkaline anion and sodium in bauxite residue through ammonium chloride treatment.The results showed that the pH of bauxite residue decreased from 10.49 to 8.93,total alkaline anion(HCO3^-,CO3^2-,OH^-,AlO2^-)concentration reduced from 38.89 to 25.50 mmol/L,leaching rate of soluble sodium was 80.86%with ammonium chloride addition of 0.75%,liquid/solid(L/S)ratio of 3(mL/g),temperature of 30°C and reaction time of 18 h;L/S ratio was the main factor affecting the removal of alkaline anion and the leaching of sodium.Furthermore,ammonium chloride promoted the dissolution of diaspore and changed the micro/morphological characteristics with the increase of massive structure.The findings of this work will contribute to achieve soil-formation of bauxite residue.
基金Project(201509050)supported by Special Program on Environmental Protection for Public Welfare,ChinaProjects(51474247,51634010)supported by the National Natural Science Foundation of ChinaProject(2015CX001)supported by Grants from the Project of Innovation-driven Plan in Central South University,China
文摘Physicochemical properties and leaching behaviors of two typical arsenic-bearing lime?ferrate sludges(ABLFS),waste acid residue(WAR)and calcium arsenate residue(CAR),are comprehensively described.The chemical composition,morphological features,phase composition and arsenic occurrence state of WAR and CAR are analyzed by ICP?AES,SEM?EDS,XRD,XPS and chemical phase analysis.The toxicity leaching test and three-stage BCR sequential extraction procedure are utilized to investigate arsenic leaching behaviors.The results show that the contents of arsenic in WAR and CAR are2.5%and21.2%and mainly present in the phases of arsenate and arsenic oxides dispersed uniformly or agglomerated in amorphous particles.The leaching concentrations of arsenic excess119and1063times of TCLP standard regulatory level with leaching rates of47.66%and50.15%for WAR and CAR,respectively.About90%of extracted arsenic is in the form of acid soluble and reducible,which is the reason of high arsenic leaching toxicity and environmental activity of ABLFS.This research provides comprehensive information on harmless disposal of ABLFS from industrial wastewater treatment of lime?ferrate process.
基金Project(41371475)supported by the National Natural Science Foundation of ChinaProject(201509048)supported by the Environmental Protection’s Special Scientific Research for Chinese Public Welfare Industry
文摘Bauxite residue is a highly alkaline waste containing soluble alkaline anions, which can cause environmental concerns. The optimal leaching conditions, distribution of alkaline anions, types of pivotal alkaline anions and their dissolution behaviors were investigated based on the combination of single factors-orthogonal experiments and leaching stage experiment. Using a two-stage leaching, 86% of the soluble alkaline anions(CO3^2-, HCO4^-,Al(OH)4^-, OH^-) were leached with a L/S ratio of 2 mL/g, at 30 ℃, over 23 h. During the first stage of leaching, approximately 88% of alkaline anions were leached from the dissolution of free alkali(Na OH, carbonate, bicarbonate, NaAl(OH)4) with the rest originating from the dissolution of alkaline minerals(calcite, cancrinite and hydrogarnet). Supernatant alkalinity was 69.78 mmol/L with CO3^2- accounting for 75%. Furthermore, carbonate leaching was controlled by solid film diffusion using the Stumm Model with an apparent activation energy of 10.24 kJ/mol.
基金Project (50964004) supported by the National Natural Science Foundation of China
文摘The leaching behavior of main metallic sulphides in zinc concentrate under atmospheric oxygen-rich direct leaching conditions was studied through mineralogical analysis. The results show that the sulphides dissolve obviously except pyrite. Based on the relationship between elemental sulfur and the residual sulphides in the leaching residue, the dissolution of sphalerite, chalcopyrite, covellite and galena is assumed to follow the indirect oxidation reactions, where the acidic dissolution takes place firstly and then the released H2S transfers from the mineral surface into bulk solution and is further oxidized into elemental sulfur. The interface chemical reaction is further supposed as the controlling step in the leaching of these sulphides. The direct electrochemical oxidation reactions are assumed to contribute to the dissolution of pyrrhotite, which is controlled by the diffusion through elemental sulfur layer.