Effects of current density on microstructure and properties of plasma electrolytic oxidation ceramic coatings formed on 6063 aluminum alloy 被引量:10
1
作者 项南 宋仁国 +3 位作者 庄俊杰 宋若希 陆筱雅 苏旭平 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2016年第3期806-813,共8页
Plasma electrolytic oxidation (PEO) ceramic coatings were fabricated in a silicate-based electrolyte with the addition of potassium fluorozirconate (K2ZrF6) on 6063 aluminum alloy, and the effects of current density o... Plasma electrolytic oxidation (PEO) ceramic coatings were fabricated in a silicate-based electrolyte with the addition of potassium fluorozirconate (K2ZrF6) on 6063 aluminum alloy, and the effects of current density on microstructure and properties of the PEO coatings were studied. It was found that pore density of the coatings decreased with increasing the current density. The tribological and hardness tests suggested that the ceramic coating produced under the current density of 15 A/dm2showed the best mechanical property, which matched well with the phase analysis. Electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization curves proved that the coating obtained under 15 A/dm2 displayed the best anti-corrosion property, which was directly connected with morphologies of coatings. 展开更多
关键词 6063 aluminum alloy ceramic coating plasma electrolytic oxidation(PEO) current density MICROSTRUCTURE mechanical property
下载PDF
Microstructure and mechanical properties of ceramic coatings formed on 6063 aluminium alloy by micro-arc oxidation 被引量:10
2
作者 项南 宋仁国 +3 位作者 赵坚 李海 王超 王芝秀 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2015年第10期3323-3328,共6页
The microstructure and mechanical properties of ceramic coatings formed on 6063 aluminium alloy obtained in silicate-,borate- and aluminate-based electrolyte without and with nanoadditive Al2O3 and TiO2 by micro-arc o... The microstructure and mechanical properties of ceramic coatings formed on 6063 aluminium alloy obtained in silicate-,borate- and aluminate-based electrolyte without and with nanoadditive Al2O3 and TiO2 by micro-arc oxidation(MAO) were studied by scanning electron microscopy(SEM),energy-dispersive X-ray spectroscopy(EDS),X-ray diffraction(XRD),microhardness and friction-abrasion tests,respectively.SEM results show that coatings with nanoadditive have less porosities than those without nanoadditive.XRD results reveal that nanoadditive-containing coatings contain more oxides compared with nanoadditive-free coatings in all cases,which are consistent with the EDS analysis.Mechanical properties tests show that nanoadditive Al2O3-containing coatings have higher microhardness values compared with the other coatings obtained in silicate-,borate- and aluminate-based electrolyte.On the other hand,nanoadditive has a positive effect on improving the wearing-resistance of MAO coatings in all cases.Furthermore,the borate-MAO coatings present an inferior anti-wearing property compared with the silicate- and aluminate-MAO coatings for both the nanoadditive-free and nanoadditive-containing coatings. 展开更多
关键词 6063 aluminium alloy micro-arc oxidation MICROSTRUCTURE mechanical properties nanoadditive
下载PDF
稀土元素在6063合金中的分布及其作用机理 被引量:11
3
作者 赵敏寿 党平 吕翔平 《中国稀土学报》 CAS CSCD 北大核心 1989年第3期59-64,共6页
用金相观察、扫描电镜的波谱和能谱分析结果表明,稀土在6063铝合金铸态组织中富集于晶界,稀土促进了Si和Fe向晶界偏聚,减少了针状铁相,铸态组织均匀、细化,强度提高。过量稀土会形成Al—La类稀土夹杂物,分布在晶界和晶内,使铸态组织粗化... 用金相观察、扫描电镜的波谱和能谱分析结果表明,稀土在6063铝合金铸态组织中富集于晶界,稀土促进了Si和Fe向晶界偏聚,减少了针状铁相,铸态组织均匀、细化,强度提高。过量稀土会形成Al—La类稀土夹杂物,分布在晶界和晶内,使铸态组织粗化,合金强度下降。含稀土的铝合金型材中铁相有所细化,稀土化合物呈球团状,强度及硬度有所提高。 展开更多
关键词 稀土元素 6063 铝合金 分布 作用
下载PDF
Corrosion Behavior of Extruded near Eutectic Al—Si—Mg and 6063 Alloys 被引量:8
4
作者 Yuna Wu Hengcheng Liao 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2013年第4期380-386,共7页
In this work, a comparison study on corrosion behavior of extruded near eutectic Al-12.3%Si-0.26%Mg and 6063 alloys has been carried out by mass loss test in 4% H2SO4 aqueous solution in the open air and potentiodynam... In this work, a comparison study on corrosion behavior of extruded near eutectic Al-12.3%Si-0.26%Mg and 6063 alloys has been carried out by mass loss test in 4% H2SO4 aqueous solution in the open air and potentiodynamic polarization test in 3.5 wt.% NaCI aqueous solution. Results indicate that the corrosion resistance of the near eutectic AI-Si-Mg alloy is less than that of 6063 alloy. Macro/microscopy and scanning electron microscopy results clearly show the difference of the corrosion progress of these two alloys in 4% H2SO4 aqueous solution. The corrosion type of 6063 alloy is pitting corrosion. The Mg2Si and AIFeSi particles and surface defects act as nucleation sites for pitting, and the amount and distribution of them have a significant effect on the pitting behavior. For the near eutectic alloy, there are two types of corrosion cells. One is between the extruded primary α-AI and the eutectic, the other is between the eutectic AI and eutectic Si particles. Combination of these two types of corrosion cells leads to a lower corrosion resistance, a higher mass loss of the near eutectic alloy compared with 6063 alloy, and the formation of the paralleling corroded grooves. 展开更多
关键词 AI-Si alloy 6063 Alloy Corrosion mechanism PITTING Microstructure Potentiodynamic polarization
原文传递
Effects of extrusion speed of continuous extrusion with double billets on welding performance of 6063 Al alloy 被引量:7
5
作者 Ying ZHAO Jiu-yang PEI +2 位作者 Li-li GUO Xin-bing YUN Huai-chao MA 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2021年第6期1561-1571,共11页
During continuous extrusion,the welds were formed at the confluence of two billets.Influences of extrusion wheel rotational speed on micromorphology and properties of welds of 6063 Al alloy were investigated through m... During continuous extrusion,the welds were formed at the confluence of two billets.Influences of extrusion wheel rotational speed on micromorphology and properties of welds of 6063 Al alloy were investigated through microstructure observation,tensile test,and SEM analyses.Welding parameters were analyzed using finite element simulation.Results indicated that metal welding was remarkably affected by oxide on outer surface of the double billets during continuous extrusion.Degree of oxide breakage on the welding surface increased due to the evident increase in effective strain rate with increasing extrusion speed.The high temperature induced by increased extrusion speed accelerated the formation of metallurgical bonding.A portion of weld seam lines slowly disappeared,and the proportion of the welding interface that failed to reach metallurgical bonding was also gradually reduced.Tensile strength and elongation of the weld specimen increased with the increase of extrusion speed. 展开更多
关键词 continuous extrusion 6063 Al alloy extrusion speed welding performance
下载PDF
Constitutive equations for high temperature flow stress prediction of 6063 Al alloy considering compensation of strain 被引量:7
6
作者 甘春雷 郑开宏 +1 位作者 戚文军 王孟君 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2014年第11期3486-3491,共6页
In order to develop the appropriate constitutive equation which can precisely model high temperature flow stress of 6063 Al alloy, a series of isothermal hot compression tests were performed at temperatures from 573 t... In order to develop the appropriate constitutive equation which can precisely model high temperature flow stress of 6063 Al alloy, a series of isothermal hot compression tests were performed at temperatures from 573 to 773 K and strain rates from 0.5 to 50 s?1 on a Gleeble?1500 thermo-simulation machine. Zener–Hollomon parameter in an exponent-type equation was used to describe the combined effects of temperature and strain rate on hot deformation behaviour of 6063 Al alloy, whereas the influence of strain was incorporated in the developed constitutive equation by considering material constants (α,n,Q andA) to be 4th order polynomial functions of strain. The results show that the developed constitutive equation can accurately predict high temperature flow stress of 6063 Al alloy, which demonstrates that it can be suitable for simulating hot deformation processes such as extrusion and forging, and for properly designing the deformation parameters in engineering practice. 展开更多
关键词 6063 Al alloy constitutive equation flow stress STRAIN hot deformation
下载PDF
Influence of heat treatment conditions on bending characteristics of 6063 aluminum alloy sheets 被引量:6
7
作者 Zhi-wen LIU Luo-xing LI +3 位作者 Jie YI Shi-kang LI Zhen-hu WANG Guan WANG 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2017年第7期1498-1506,共9页
Bending deformation behaviors of solution treated(ST),natural aged(NA)and T6tempered6063aluminum alloy sheetswere studied by three-point bending tests.The changes of bending force,interior angle,bending radius and she... Bending deformation behaviors of solution treated(ST),natural aged(NA)and T6tempered6063aluminum alloy sheetswere studied by three-point bending tests.The changes of bending force,interior angle,bending radius and sheet thickness in thefillet region were analyzed by experimental measurements and numerical simulations.The results showed that the bendingcharacteristics were strongly dependent on the heat treatment conditions.The T6alloy sheets were bent more sharply and localplastic deformation occurred severely in the fillet region.However,the ST and NA alloy sheets exhibited relatively uniform bendingdeformation and large bending radius.The bending force of T6alloy was the highest,followed by the NA alloy and that of the STalloy was minimum.After unloading,as compared with the ST and NA alloys,the springback of T6alloys was markedly larger.Theaging time showed a positive sensitivity on the springback and non-uniform bending deformability.The bending characteristics areattributed to the combined effects of yield strength,yield ratio and coefficient of neutral layer. 展开更多
关键词 6063 aluminum alloy three-point bending heat treatment conditions bending characteristic yield ratio simulation
下载PDF
Time-temperature-property curves for quench sensitivity of 6063 aluminum alloy 被引量:6
8
作者 李红英 曾翠婷 +2 位作者 韩茂盛 刘蛟蛟 鲁晓超 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第1期38-45,共8页
The quench sensitivity of 6063 alloy was investigated via constructing time-temperature-property(TTP) curves by interrupted quenching technique and transmission electron microscopy(TEM) analysis.The results show t... The quench sensitivity of 6063 alloy was investigated via constructing time-temperature-property(TTP) curves by interrupted quenching technique and transmission electron microscopy(TEM) analysis.The results show that the quench sensitivity of 6063 alloy is lower than that of 6061 or 6082 alloy,and the critical temperature ranges from 300 to 410℃ with the nose temperature of about 360℃.From TEM analysis,heterogeneous precipitate β-Mg2Si is prior to nucleate on the(AlxFeySiz) dispersoids in the critical temperature range,and grows up most rapidly at the nose temperature of 360℃.The heterogeneous precipitation leads to a low concentration of solute,which consequently reduces the amount of the strengthening phase β'' after aging.In the large-scale industrial production of 6063 alloy,the cooling rate during quenching should be enhanced as high as possible in the quenching sensitive temperature range(410-300℃) to suppress the heterogeneous precipitation to get optimal mechanical properties,and it should be slowed down properly from the solution temperature to 410℃ and below 300℃ to reduce the residual stress. 展开更多
关键词 6063 aluminum alloy quench sensitivity HARDNESS time-temperature-property curve strengthening phase heterogeneous precipitation residual stress
下载PDF
Influence of dynamic recrystallization on microstructure and mechanical properties of welding zone in Al-Mg-Si aluminum profile during porthole die extrusion 被引量:5
9
作者 Shi-kang LI Luo-xing LI +2 位作者 Hong HE Zhi-wen LIU Long ZHANG 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2019年第9期1803-1815,共13页
The effect of dynamic recrystallization(DRX)on the microstructure and mechanical properties of 6063 aluminum alloy profile during porthole die extrusion was studied through experiment and simulation.The grain morpholo... The effect of dynamic recrystallization(DRX)on the microstructure and mechanical properties of 6063 aluminum alloy profile during porthole die extrusion was studied through experiment and simulation.The grain morphology was observed by means of electron backscatter diffraction(EBSD)technology.The results show that,at low ram speeds,increasing the ram speed caused an increase in DRX fraction due to the increase of temperature and strain rate.In contrast,at high ram speeds,further increasing ram speed had much less effect on the temperature,and the DRX faction decreased due to high stain rates.The microhardness and fraction of low angle boundaries in the welding zones were lower than those in the matrix zones.The grain size in the welding zone was smaller than that in the matrix zone due to lower DRX fraction.The decrease of grain size and increase of extrudate temperature were beneficial to the improvement of microhardness. 展开更多
关键词 6063 aluminum alloy porthole die extrusion dynamic recrystallization MICROSTRUCTURE mechanical properties
下载PDF
电导率与铝合金挤压制程稳定性的研究 被引量:6
10
作者 丁小理 高森田 《铝加工》 CAS 2016年第2期45-49,共5页
铝合金的化学成分、加工及热处理状态等与其电导率有一定的关联。一般而言,合金元素愈多,电导率愈低或电阻愈高。铝的合金元素在固溶状态和析出状态下,电导率不同,同属析出状态下,析出颗粒越大,电导率越高。相同铝合金的化学成分通过电... 铝合金的化学成分、加工及热处理状态等与其电导率有一定的关联。一般而言,合金元素愈多,电导率愈低或电阻愈高。铝的合金元素在固溶状态和析出状态下,电导率不同,同属析出状态下,析出颗粒越大,电导率越高。相同铝合金的化学成分通过电导率的测定,可以初步推测热处理加工状态以及某些力学性能,达到检测快速便捷的目的,从而可以判断制程的稳定性。本研究结果显示:电导率的检测是目前判定铝合金挤压制程及生产设备稳定性的最简单最实用的方法之一,半成品及成品的电导率是产品质量与制程稳定性的指标。 展开更多
关键词 铝合金 电导率 热处理 析出物 挤压制程 时效
下载PDF
Corrosion Behavior of Alumina Reinforced Aluminium (6063) Metal Matrix Composites 被引量:3
11
作者 K. K. Alaneme M. O. Bodunrin 《Journal of Minerals and Materials Characterization and Engineering》 2011年第12期1153-1165,共13页
The influence of alumina volume percent and solution heat-treatment on the corrosion behaviour of Al (6063) composites and its monolithic alloy in salt water, basic and acidic environments is investigated. Al (6063) ... The influence of alumina volume percent and solution heat-treatment on the corrosion behaviour of Al (6063) composites and its monolithic alloy in salt water, basic and acidic environments is investigated. Al (6063) – Al2O3 particulate composites containing 6, 9, 15, and 18 volume percent alumina were produced by adopting two step stir casting. Mass loss and corrosion rate measurements were utilized as criteria for evaluating the corrosion behaviour of the composites. It is observed that Al (6063) – Al2O3 composites exhibited excellent corrosion resistance in NaCl medium than in the NaOH and H2SO4 media. The unreinforced alloy exhibited slightly superior corrosion resistance than the composites in NaCl and NaOH media but the composites had better corrosion resistance in H2SO4 medium. Furthermore, solution heat-treatment resulted in improved corrosion resistance for both the composites and the unreinforced alloy while the effect of volume percent alumina on corrosion resistance did not follow a consistent trend. 展开更多
关键词 STIR CASTING Al (6063) AL2O3 composite solution heat-treatment Corrosion rate mass LOSS
下载PDF
Quantitative analysis of orange peel during tension of 6063 alloy spun tubes 被引量:3
12
作者 Yang CAI Xiao-song WANG Shi-jian YUAN 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2018年第5期858-865,共8页
Severe surface roughening during plastic deforming of aluminum alloy parts can produce "orange peel" defects. To analyze "orange peel" of 6063 aluminum alloy tube quantificationally, the tensile tests of trapezoid... Severe surface roughening during plastic deforming of aluminum alloy parts can produce "orange peel" defects. To analyze "orange peel" of 6063 aluminum alloy tube quantificationally, the tensile tests of trapezoidal specimens were carried out. The tubes with different grain sizes were obtained by spinning and subsequent annealing heat treatment. The macroscopical behavior of surface roughening was characterized by surface roughness Ra using a laser scanning confocal microscope. The corresponding microscopic behavior was reflected by microstructures of specimens and in-situ observation using electron back-scattered diffraction(EBSD). The obtained results show that the surface roughness increased firstly with increasing strain and then decreased slightly. There was a critical strain for aluminum alloy tube, below which "orange peel" defect would not occur. For the tube with a mean grain size of 80, 105, 130 and 175 μm, the critical strains were 10.17%, 5.74%, 3.15% and 1.62%, respectively. Meanwhile, the surface roughening behavior was produced by serious inhomogeneous deformation between grains as strain increased, and was aggravated as the grain size increased due to the larger local deformation in larger grains. 展开更多
关键词 6063 aluminum alloy surface roughening tensile deformation SPINNING orange peel
下载PDF
热喷涂镍粉在SUS304及A6063基体上的沉积行为 被引量:3
13
作者 杨焜 邓畅光 +1 位作者 刘敏 福本昌宏 《中国表面工程》 EI CAS CSCD 北大核心 2013年第6期18-23,共6页
为阐明基体材料对单个颗粒沉积行为的影响,采用大气等离子喷涂技术将镍粉喷涂到镜面研磨后的不锈钢SUS304及铝合金A6063基体上,并通过扫描电子显微镜及聚焦离子束等技术观察在基体上收集的沉积物正面及截面形貌。结果表明:Ni在SUS304基... 为阐明基体材料对单个颗粒沉积行为的影响,采用大气等离子喷涂技术将镍粉喷涂到镜面研磨后的不锈钢SUS304及铝合金A6063基体上,并通过扫描电子显微镜及聚焦离子束等技术观察在基体上收集的沉积物正面及截面形貌。结果表明:Ni在SUS304基体上呈明显的溅射沉积,单个沉积物的中心部位与周围溅射物相分离,沉积物底部及内部均可见明显气孔,溅射可能是由基体表面的吸附质在熔滴在基体表面铺展过程中脱附所导致。同时,Ni粉在A6063基体上呈现花朵状溅射,中心部位有明显的分层现象,这可能与基体材料的热导率、熔点以及基体表面吸附质的脱附等因素密切相关。 展开更多
关键词 热喷涂 基体材料 SUS304 A6063 沉积物形貌
下载PDF
Damage and fracture mechanism of 6063 aluminum alloy under three kinds of stress states 被引量:2
14
作者 ZHU Hao ZHU Liang CHEN Jianhong 《Rare Metals》 SCIE EI CAS CSCD 2008年第1期64-69,共6页
To study the damage and fracture mechanism of 6063 aluminum alloy under different stress states,three kinds of representative triaxial stress states have been adopted,namely smooth tensile,notch tensile,and pure shear... To study the damage and fracture mechanism of 6063 aluminum alloy under different stress states,three kinds of representative triaxial stress states have been adopted,namely smooth tensile,notch tensile,and pure shear.The results of the study indicate the following.During the notch tensile test,a relatively higher stress triaxiality appears in the root of the notch.With the applied loading increasing,the volume fraction of microvoids in the root of the notch increases continuously.When it reaches the critical volume fraction of microvoids,the specimen fractures.During the pure shear test,the stress triaxiality almost equals to zero,and there is almost no microvoids but a shear band at the center of the butterfly specimen.The shear band results from nonuniform deformation constantly under the shear stress.With stress concentration,cracks are produced within the shear band and are later coalesced.When the equivalent plastic strain reaches the critical value(equivalent plastic fracture strain),the butterfly specimen fractures.During the smooth tensile test,the stress triaxiality in the gauge of the specimen remains constant at 0.33.Thus,the volume of microvoids of the smooth tensile test is less than that of the notch tensile test and the smooth specimen fractures due to shearing between microvoids.The G-T-N damage model and Johnson-Cook model are used to simulate the notch tensile and shear test,respectively.The simulated engineering stress-strain curves fit the measured engineering stress-strain curves very well.In addition,the empirical damage evolution equation for the notch specimen is obtained from the experimental data and FEM simulations. 展开更多
关键词 6063 aluminum alloy damage mechanism fracture mechanism G-T-N model Johnson-Cook model
下载PDF
Deformation simulation of low-temperature high-speed extrusion for 6063 Al alloy 被引量:2
15
作者 王孟君 何钊 +2 位作者 武星星 李彩文 李光耀 《Journal of Central South University》 SCIE EI CAS 2010年第5期881-887,共7页
The hot compression test of 6063 Al alloy was performed on a Gleeble-1500 thermo-simulation machine, and the forming of 6063 rod cxtrudate in low-temperature high-speed extrusion was simulated with extrusion ratio of ... The hot compression test of 6063 Al alloy was performed on a Gleeble-1500 thermo-simulation machine, and the forming of 6063 rod cxtrudate in low-temperature high-speed extrusion was simulated with extrusion ratio of 25 on the platform of DEFORM 2D successfully. From the compression experimental results, the flow stress model of this Al alloy is obtained which could be the constitutive equation in the simulation of low-temperature high-speed extrusion process. From the numerical simulation results, there is a higher strain concentration at the entrance of the die and the exit temperature reaches up to 522 ℃ in low-temperature high-speed extrusion, which approaches to the quenching temperature of the 6063 Al alloy. The results show that the low-temperature high-speed extrusion method as a promsing one can reduce energy consumption effectively. 展开更多
关键词 6063 Al alloy hot deformation low-temperature high-speed extrusion constitutive equation numerical simulation
下载PDF
Si、Mg、Fe含量对6063铝合金抗拉强度、导电性能的影响 被引量:2
16
作者 李思 《电工材料》 CAS 2019年第2期3-6,17,共5页
利用DOE全因子试验设计法研究Si、Mg、Fe含量在规定范围内配比的变化对T6态6063合金的抗拉强度、导电性能的影响。结果表明:当Si含量为0.6%、Mg含量为0.9%、Fe含量为0%时,合金抗拉强度最佳。并利用Minitab软件拟合出用于计算6063合金抗... 利用DOE全因子试验设计法研究Si、Mg、Fe含量在规定范围内配比的变化对T6态6063合金的抗拉强度、导电性能的影响。结果表明:当Si含量为0.6%、Mg含量为0.9%、Fe含量为0%时,合金抗拉强度最佳。并利用Minitab软件拟合出用于计算6063合金抗拉强度的数学模型指导熔炼配料。Si、Mg含量越低,合金的导电性能越好。 展开更多
关键词 6063 合金元素 抗拉强度 导电性能
下载PDF
Deformation Behavior of 6063 Aluminum Alloy During High-Speed Compression 被引量:2
17
作者 王孟君 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2005年第3期40-43,共4页
The deformation behavior characteristics of 6063 aluminum alloy were studied experimentally by isothermal compression tests on a Gleeble- 1500 thermal-mechanical simulator. Cylindrical specimens of 14mm in height and ... The deformation behavior characteristics of 6063 aluminum alloy were studied experimentally by isothermal compression tests on a Gleeble- 1500 thermal-mechanical simulator. Cylindrical specimens of 14mm in height and 10mm in diameter were compressed dynamically at temperatures ranging from 473 to 723K and at higher strain rntes from 5 to 30s^-1. It is fouud that the flow curves not only depend on the strain rate and temperature but nlso on the dynamic recovery aud recrystallization behavior. The results show that the flow stress decreased with the increase of temperature, while increased with the increase of strain rate. The discontinuous dynamic recrystallization (DDRX) may take place at a high strain rate of 20s^-1 under the tested conditions. At 30s^-1 , the flow curve can exhibit,flow softening due to the effect of temperature rise that raised the temperature by aboat 32K in less than 0.05s. 展开更多
关键词 6063 Al alloy flow stress dynamic recovery discontinuous dynamic recrystallization temperature rise
下载PDF
Formation and elimination of burst phenomenon in ultrasonic-assisted resistance brazing 被引量:1
18
作者 Wei-yuan YU Tian-yu ZHANG +5 位作者 Yu WANG Meng-zhao GAO Jiang-xu SHANG Ze-hua YAN Wei-jie WU Qiao-li LIN 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2019年第3期485-494,共10页
A two-step ultrasonic-assisted brazing method and its associated apparatus were developed to make 6063 aluminum alloys joints with Al-Si-Mg filler metal. The burst phenomenon and the effect of ultrasonic direction and... A two-step ultrasonic-assisted brazing method and its associated apparatus were developed to make 6063 aluminum alloys joints with Al-Si-Mg filler metal. The burst phenomenon and the effect of ultrasonic direction and time, as well as the welding joint geometry on the burst phenomenon were investigated. The results show that the burst phenomenon occurs in the liquid filler metal under the effects of high current density, heat, and interaction force. The burst phenomenon is eliminated when the oxide film on the edge of the cross-section of the two parent metals is removed with more than or equal to 6 s ultrasonic time. A model of formation and elimination for burst was proposed, through which the blasting phenomenon can be controlled by changing the ultrasonic time and the geometrical shape of the welded joint. 展开更多
关键词 6063 aluminum alloys ultrasonic-assisted brazing resistance brazing BURST
下载PDF
Effect of Current Density on Microstructure and Corrosion Behavior of Plasma Electrolytic Oxidation Coated 6063 Aluminum Alloy 被引量:1
19
作者 ZHUANG Junjie SONG Renguo 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2018年第6期1503-1510,共8页
Plasma electrolytic oxidation(PEO) coatings were fabricated on 6063 aluminum alloy in a cheap and convenient electrolyte. The effect of different current densities, i e, 5, 10, 15, and 20 A/dm2on the microstructure an... Plasma electrolytic oxidation(PEO) coatings were fabricated on 6063 aluminum alloy in a cheap and convenient electrolyte. The effect of different current densities, i e, 5, 10, 15, and 20 A/dm2on the microstructure and corrosion behavior of coatings was comprehensively studied by scanning electron microscopy(SEM), stereoscopic microscopy, potentiodynamic polarization and electrochemical impedance spectroscopy(EIS), respectively. It is found that the pore density decreases and the pore size increases with increasing current density. The XRD results show that the coatings are only composed of α-Al2O3and γ-Al2O3. Potentiodynamic polarization test proves that the coating formed under 10 A/dm2possesses the best anticorrosion property. The long time EIS test shows that the coating under 10 A/dm2is able to protect the aluminum alloy substrate after long time of immersion in 0.59 M NaCl solution, which confirms the salt solution immersion test results in 2 M NaCl solution. 展开更多
关键词 COATING 6063 aluminum alloy plasma electrolytic oxidation (PEO) current density corrosion resistance
下载PDF
A Comparative Study on the Milling Speed for the Synthesis of Nano-Structured Al 6063 Alloy Powder by Mechanical Alloying
20
作者 Hafeez Ahamed V. Senthil Kumar 《Journal of Minerals and Materials Characterization and Engineering》 2011年第6期507-515,共9页
The present article reports on characterization studies performed on amorphized nanostructured Al 6063 alloy powder synthesized by mechanical alloying (MA). The as-milled powder was characterized by X-ray diffraction ... The present article reports on characterization studies performed on amorphized nanostructured Al 6063 alloy powder synthesized by mechanical alloying (MA). The as-milled powder was characterized by X-ray diffraction (XRD) for investigating the development of crystallite nature and determining the different phases of the materials present, scanning electron microscope (SEM) was used for in depth morphological study and High Resolution-transmission electron microscope (HR-TEM) was employed to ensure the development of a nano-structured nature of the Al 6063 matrix. In the present work alloyed powder was milled for 20 h and 40 h at 300 rpm;and 20 h at 700 rpm in a hardened stainless steel medium. Using Williamson-Hall equation;crystallite size, lattice strain and lattice parameter of Al 6063 nanostructure alloy powder was estimated with broadening of XRD peaks. XRD results showed that the crystallite size of Al 6063 alloy powder reached 32 and 53 nm after 20 h at 700 rpm and 40 h at 300 rpm respectively. 展开更多
关键词 Nano-structured AL 6063 Synthesis.