The high compacted density LiNi<sub>0.5-x</sub>Co<sub>0.2</sub>Mn<sub>0.3</sub>Mg<sub>x</sub>O<sub>2</sub> cathode material for lithium-ion batteries was syn...The high compacted density LiNi<sub>0.5-x</sub>Co<sub>0.2</sub>Mn<sub>0.3</sub>Mg<sub>x</sub>O<sub>2</sub> cathode material for lithium-ion batteries was synthesized by high temperature solid-state method, taking the Mg element as a doping element and the spherical Ni<sub>0.5</sub>Co<sub>0.2</sub>Mn<sub>0.3</sub> (OH)<sub>2</sub>, Li<sub>2</sub>CO<sub>3</sub> as raw materials. The effects of calcination temperature on the structure and properties of the products were investigated. The structure and morphology of cathode materials powder were analyzed by X-ray diffraction spectroscopy (XRD) and scanning electronmicroscopy (SEM). The electrochemical properties of the cathode materials were studied by charge-discharge test and cyclic properties test. The results show that LiNi<sub>0.4985</sub>Co<sub>0.2</sub>Mn<sub>0.3</sub> Mg<sub>0.0015</sub>O<sub>2</sub> cathode material prepared at calcination temperature 930°C has a good layered structure, and the compacted density of the electrode sheet is above 3.68 g/cm<sup>3</sup>. The discharge capacity retention rate is more than 97.5% after 100 cycles at a charge-discharge rate of 1C, displaying a good cyclic performance.展开更多
The discovery of ferromagnetic two-dimensional(2D)van der Waals(vdWs)materials provides an opportunity to explore intriguing physics and to develop innovative spin electronic devices.However,the main challenge for pra...The discovery of ferromagnetic two-dimensional(2D)van der Waals(vdWs)materials provides an opportunity to explore intriguing physics and to develop innovative spin electronic devices.However,the main challenge for practical applications of vd Ws ferromagnetic crystals lies in the weak intrinsic ferromagnetism and small perpendicular magnetic anisotropy(PMA)above room temperature.Here,we report the intrinsic vd Ws ferromagnetic crystal Fe_(3)GaTe_(2),synthesized by the self-flux method,exhibiting a Curie temperature(TC)of 370 K,a high saturation magnetization of 33.47 emu/g,and a large PMA energy density of approximately 4.17×10^(5)J/m^(3).Furthermore,the magneto-optical effect is systematically investigated in Fe_(3)GaTe_(2).The doubly degenerate E_(2g)(Γ)mode reverses the helicity of incident photons,indicating the existence of pseudoangular-momentum(PAM)and chirality.Meanwhile,the non-degenerate non-chiral A_(1g)(Γ)phonon exhibits a significant magneto-Raman effect under an external out-of-plane magnetic field.These results lay the groundwork for studying phonon chirality and magneto-optical phenomena in 2D magnetic materials,providing the feasibility for further fundamental research and applications in spintronic devices.展开更多
一氧化氮电还原反应将工业废气转化为有价值的氨,表现出极具潜力的应用前景.在本工作中,我们合成了具有高比表面积和丰富缺陷的氧化铜纳米片催化剂,在流动池中氨法拉第效率达到92.1%,在-0.2 V vs.RHE时,一氧化氮电还原电流密度和氨的生...一氧化氮电还原反应将工业废气转化为有价值的氨,表现出极具潜力的应用前景.在本工作中,我们合成了具有高比表面积和丰富缺陷的氧化铜纳米片催化剂,在流动池中氨法拉第效率达到92.1%,在-0.2 V vs.RHE时,一氧化氮电还原电流密度和氨的生产速率分别达到1.1 A cm^(-2)和7356μmol cm^(-2)h^(-1).在电流密度超过400 m A cm-2时,氨法拉第效率在50小时保持在80%以上.准原位X射线光电子能谱和原位X射线吸收光谱结果表明氧化铜纳米片在一氧化氮电还原过程中被电化学还原成单质铜.与铜纳米颗粒相比,氧化铜纳米片展现出较高的电化学表面积和一氧化氮电还原的内在活性.展开更多
The emergent van der Waals magnetic material is a promising component for spintronic devices with novel functionalities.Here,we report a transition of negative-to-positive magnetoresistance in Fe_(3)GeTe_(2)/Cr_(2)Ge_...The emergent van der Waals magnetic material is a promising component for spintronic devices with novel functionalities.Here,we report a transition of negative-to-positive magnetoresistance in Fe_(3)GeTe_(2)/Cr_(2)Ge_(2)Te_(6)/Fe_(3)GeTe_(2)van der Waals all-magnetic tunnel junctions with increasing the applied bias voltage.A negative magnetoresistance is observed first in Fe_(3)GeTe_(2)/Cr_(2)Ge_(2)Te_(6)/Fe_(3)GeTe_(2)tunnel junctions,where the resistance with antiparallel aligned magnetization of two Fe_(3)GeTe_(2)electrodes is lower than that with parallel alignment,which is due to the opposite spin polarizations of two Fe_(3)GeTe_(2)electrodes.With the bias voltage increasing,the spin polarization of the biased Fe_(3)GeTe_(2)electrode is changed so that the spin orientations of two Fe_(3)GeTe_(2)electrodes are the same.Our experimental observations are supported by the calculated spin-dependent density of states for Fe_(3)GeTe_(2)electrodes under a finite bias.The significantly bias voltage-dependent spin transport properties in van der Waals magnetic tunnel junctions open a promising route for designing electrical controllable spintronic devices based on van der Waals magnets.展开更多
The reservoir thickness of sub-member of Lower Permain in the south of the eastern margin of Ordos Basin is thin and large variable i laterally. And the seismic response characteristics of sandstone reservoir are doub...The reservoir thickness of sub-member of Lower Permain in the south of the eastern margin of Ordos Basin is thin and large variable i laterally. And the seismic response characteristics of sandstone reservoir are doubly interfered by the strong reflection sidelobes of overlying 5# coal seam and underlying 8# coal seam. In view of this situation, in order to better eliminate the influence of upper and lower coal seams and improve the accuracy of reservoir prediction, the strategy of de-strong seismic reflection and de-logging (curve) interference is adopted to carry out the matching of logging and seismic, and on this basis, uses the seismic waveform indication inversion to predict the thin sandstone. The steps are as follows: firstly, by using wavelet decomposition and reconstruction technology, select the seismic wavelet component that can better characterize the reservoir or oil & gas to reasonablely reconstruct seismic data, weaken the influence of the strong reflection from overlying 5# coal seam and underlying 8# coal seam, and highlight the response of weak seismic reflection of tight sandstone in Shan 2<sup>3</sup> sub-member;Then, the acoustic value of coal seam is corrected to that of mudstone on the logging curve to maintain the consistency of logseismic data. This method realizes the effective identification of sandstone reservoir in Shan 2<sup>3</sup> sub-member, and greatly improves the target-penetrated rate and sandstone-penetrated rate of horizontal wells.展开更多
文摘The high compacted density LiNi<sub>0.5-x</sub>Co<sub>0.2</sub>Mn<sub>0.3</sub>Mg<sub>x</sub>O<sub>2</sub> cathode material for lithium-ion batteries was synthesized by high temperature solid-state method, taking the Mg element as a doping element and the spherical Ni<sub>0.5</sub>Co<sub>0.2</sub>Mn<sub>0.3</sub> (OH)<sub>2</sub>, Li<sub>2</sub>CO<sub>3</sub> as raw materials. The effects of calcination temperature on the structure and properties of the products were investigated. The structure and morphology of cathode materials powder were analyzed by X-ray diffraction spectroscopy (XRD) and scanning electronmicroscopy (SEM). The electrochemical properties of the cathode materials were studied by charge-discharge test and cyclic properties test. The results show that LiNi<sub>0.4985</sub>Co<sub>0.2</sub>Mn<sub>0.3</sub> Mg<sub>0.0015</sub>O<sub>2</sub> cathode material prepared at calcination temperature 930°C has a good layered structure, and the compacted density of the electrode sheet is above 3.68 g/cm<sup>3</sup>. The discharge capacity retention rate is more than 97.5% after 100 cycles at a charge-discharge rate of 1C, displaying a good cyclic performance.
基金supported by the National Key Research and Development Program of China(Grant No.2022YFA1405100)the Beijing Natural Science Foundation Key Program(Grant No.Z220005)the National Natural Science Foundation of China(Grant Nos.12241405,12174384,and 12204058)。
文摘The discovery of ferromagnetic two-dimensional(2D)van der Waals(vdWs)materials provides an opportunity to explore intriguing physics and to develop innovative spin electronic devices.However,the main challenge for practical applications of vd Ws ferromagnetic crystals lies in the weak intrinsic ferromagnetism and small perpendicular magnetic anisotropy(PMA)above room temperature.Here,we report the intrinsic vd Ws ferromagnetic crystal Fe_(3)GaTe_(2),synthesized by the self-flux method,exhibiting a Curie temperature(TC)of 370 K,a high saturation magnetization of 33.47 emu/g,and a large PMA energy density of approximately 4.17×10^(5)J/m^(3).Furthermore,the magneto-optical effect is systematically investigated in Fe_(3)GaTe_(2).The doubly degenerate E_(2g)(Γ)mode reverses the helicity of incident photons,indicating the existence of pseudoangular-momentum(PAM)and chirality.Meanwhile,the non-degenerate non-chiral A_(1g)(Γ)phonon exhibits a significant magneto-Raman effect under an external out-of-plane magnetic field.These results lay the groundwork for studying phonon chirality and magneto-optical phenomena in 2D magnetic materials,providing the feasibility for further fundamental research and applications in spintronic devices.
基金supported by the National Key R&D Program of China (2023YFA1508002)the National Natural Science Foundation of China (22125205 and 92015302)+2 种基金the Fundamental Research Funds for the Central Universities (20720220008)Dalian National Laboratory for Clean Energy (DNL201923)the Photon Science Center for Carbon Neutrality。
文摘一氧化氮电还原反应将工业废气转化为有价值的氨,表现出极具潜力的应用前景.在本工作中,我们合成了具有高比表面积和丰富缺陷的氧化铜纳米片催化剂,在流动池中氨法拉第效率达到92.1%,在-0.2 V vs.RHE时,一氧化氮电还原电流密度和氨的生产速率分别达到1.1 A cm^(-2)和7356μmol cm^(-2)h^(-1).在电流密度超过400 m A cm-2时,氨法拉第效率在50小时保持在80%以上.准原位X射线光电子能谱和原位X射线吸收光谱结果表明氧化铜纳米片在一氧化氮电还原过程中被电化学还原成单质铜.与铜纳米颗粒相比,氧化铜纳米片展现出较高的电化学表面积和一氧化氮电还原的内在活性.
基金supported by the National Key Research and Development Program of China(Grant No.2022YFA1405100)the Beijing Natural Science Foundation Key Program(Grant No.Z190007)+1 种基金the Strategic Priority Research Program of Chinese Academy of Sciences(Grant Nos.XDB44000000 and XDB28000000)the National Natural Science Foundation of China(Grant Nos.12241405,11734004,and 12174028)。
文摘The emergent van der Waals magnetic material is a promising component for spintronic devices with novel functionalities.Here,we report a transition of negative-to-positive magnetoresistance in Fe_(3)GeTe_(2)/Cr_(2)Ge_(2)Te_(6)/Fe_(3)GeTe_(2)van der Waals all-magnetic tunnel junctions with increasing the applied bias voltage.A negative magnetoresistance is observed first in Fe_(3)GeTe_(2)/Cr_(2)Ge_(2)Te_(6)/Fe_(3)GeTe_(2)tunnel junctions,where the resistance with antiparallel aligned magnetization of two Fe_(3)GeTe_(2)electrodes is lower than that with parallel alignment,which is due to the opposite spin polarizations of two Fe_(3)GeTe_(2)electrodes.With the bias voltage increasing,the spin polarization of the biased Fe_(3)GeTe_(2)electrode is changed so that the spin orientations of two Fe_(3)GeTe_(2)electrodes are the same.Our experimental observations are supported by the calculated spin-dependent density of states for Fe_(3)GeTe_(2)electrodes under a finite bias.The significantly bias voltage-dependent spin transport properties in van der Waals magnetic tunnel junctions open a promising route for designing electrical controllable spintronic devices based on van der Waals magnets.
文摘The reservoir thickness of sub-member of Lower Permain in the south of the eastern margin of Ordos Basin is thin and large variable i laterally. And the seismic response characteristics of sandstone reservoir are doubly interfered by the strong reflection sidelobes of overlying 5# coal seam and underlying 8# coal seam. In view of this situation, in order to better eliminate the influence of upper and lower coal seams and improve the accuracy of reservoir prediction, the strategy of de-strong seismic reflection and de-logging (curve) interference is adopted to carry out the matching of logging and seismic, and on this basis, uses the seismic waveform indication inversion to predict the thin sandstone. The steps are as follows: firstly, by using wavelet decomposition and reconstruction technology, select the seismic wavelet component that can better characterize the reservoir or oil & gas to reasonablely reconstruct seismic data, weaken the influence of the strong reflection from overlying 5# coal seam and underlying 8# coal seam, and highlight the response of weak seismic reflection of tight sandstone in Shan 2<sup>3</sup> sub-member;Then, the acoustic value of coal seam is corrected to that of mudstone on the logging curve to maintain the consistency of logseismic data. This method realizes the effective identification of sandstone reservoir in Shan 2<sup>3</sup> sub-member, and greatly improves the target-penetrated rate and sandstone-penetrated rate of horizontal wells.