After compositing with SiO_2 layers, it is shown that superlattice-like Sb/SiO_2 thin films have higher crystallization temperature(~240°C), larger crystallization activation energy(6.22 e V), and better data...After compositing with SiO_2 layers, it is shown that superlattice-like Sb/SiO_2 thin films have higher crystallization temperature(~240°C), larger crystallization activation energy(6.22 e V), and better data retention ability(189°C for 10 y). The crystallization of Sb in superlattice-like Sb/SiO_2 thin films is restrained by the multilayer interfaces. The reversible resistance transition can be achieved by an electric pulse as short as 8 ns for the Sb(3 nm)/SiO_2(7 nm)-based phase change memory cell. A lower operation power consumption of 0.09 m W and a good endurance of 3.0 × 10~6 cycles are achieved. In addition, the superlattice-like Sb(3 nm)/SiO_2(7 nm) thin film shows a low thermal conductivity of 0.13 W/(m·K).展开更多
基金Supported by the National Natural Science Foundation of China under Grant No 11774438the Natural Science Foundation of Jiangsu Province under Grant No BK20151172+2 种基金the Changzhou Science and Technology Bureau under Grant No CJ20160028the Qing Lan Project,the Opening Project of State Key Laboratory of Silicon Materials under Grant No SKL2017-04the Opening Project of Key Laboratory of Microelectronic Devices and Integrated Technology of Institute of Microelectronics of Chinese Academy of Sciences
文摘After compositing with SiO_2 layers, it is shown that superlattice-like Sb/SiO_2 thin films have higher crystallization temperature(~240°C), larger crystallization activation energy(6.22 e V), and better data retention ability(189°C for 10 y). The crystallization of Sb in superlattice-like Sb/SiO_2 thin films is restrained by the multilayer interfaces. The reversible resistance transition can be achieved by an electric pulse as short as 8 ns for the Sb(3 nm)/SiO_2(7 nm)-based phase change memory cell. A lower operation power consumption of 0.09 m W and a good endurance of 3.0 × 10~6 cycles are achieved. In addition, the superlattice-like Sb(3 nm)/SiO_2(7 nm) thin film shows a low thermal conductivity of 0.13 W/(m·K).